MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Manifattura Cattaneo VESPEL® SP1 Polyimide
Categories: Polymer; Thermoplastic; Polyimide, Thermoplastic

Material Notes: Manifattura Cattaneo products are available in semi-finished forms such as bars, profiles, sheets and plates.

Information provided by Manifattura Cattaneo s.p.a.

Key Words: DuPont™ VESPEL®
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.43 g/cc0.0517 lb/in³ASTM D792
Moisture Absorption at Equilibrium 1.0 - 1.3 %
@Temperature 23.0 °C
1.0 - 1.3 %
@Temperature 73.4 °F
50% RH; ASTM D570
Water Absorption at Saturation 0.72 %0.72 %ASTM D570
Deformation 1.0 %
@Time 86400 sec,
Pressure 100 MPa
1.0 %
@Time 24.0 hour,
Pressure 14500 psi
ASTM D621
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 86.0 MPa12500 psiASTM D638
Elongation at Break 7.5 %7.5 %ASTM D638
Flexural Strength 110 MPa16000 psiASTM D790
Compressive Yield Strength 24.8 MPa
@Strain 1 %,
Time 3.60e+6 sec
3600 psi
@Strain 1 %,
Time 1000 hour
ASTM D695
Compressive Modulus 2.413 GPa350.0 ksiASTM D695
Poissons Ratio 0.410.41
Izod Impact, Notched (ISO) 0.0430 kJ/m²0.0205 ft-lb/in²ASTM D256
Izod Impact, Unnotched (ISO) 0.750 kJ/m²0.357 ft-lb/in²ASTM D256
Coefficient of Friction, Dynamic 0.290.29on polished steel; MPC Test
Coefficient of Friction, Static 0.350.35on polished steel; MPC Test
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+16 ohm-cm>= 1.00e+16 ohm-cmASTM D257
Surface Resistance >= 1.00e+15 ohm>= 1.00e+15 ohmASTM D257
Dielectric Constant 3.55
@Frequency 1e+6 Hz
3.55
@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 22.0 kV/mm
@Thickness 2.00 mm
559 kV/in
@Thickness 0.0787 in
ASTM D149
Dielectric Loss Index 0.0034
@Frequency 1e+6 Hz
0.0034
@Frequency 1e+6 Hz
ASTM D150
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 54.0 µm/m-°C
@Temperature 23.0 - 100 °C
30.0 µin/in-°F
@Temperature 73.4 - 212 °F
Thermal Conductivity 0.350 W/m-K2.43 BTU-in/hr-ft²-°FASTM D177
Maximum Service Temperature, Air 395 °C743 °F
Deflection Temperature at 1.8 MPa (264 psi) 360 °C680 °FASTM D648-45
Flammability, UL94 V-0V-0
Oxygen Index 53 %53 %ASTM D2863
 
Compliance PropertiesMetricEnglishComments
FDA NoNo
 
Descriptive Properties
ColorBrown
UV ResistanceN

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Daelim H&L Plavis N Aromatic Polyimide, Non-Filled, Machined Parts
DuPont Mobility and Materials Vespel® SP-1 Polyimide, Machined
DuPont Mobility and Materials Vespel® SP-1 ISO Polyimide
DuPont Mobility and Materials Vespel® SP-1 Polyimide, Direct formed
Manifattura Cattaneo VESPEL® SP21 Polyimide

PMANIF916 / 156196

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.