MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Seals Eastern 7065 Neoprene / Chloroprene
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: General purpose neoprene

Information provided by Seals Eastern, Inc.

Key Words: Polychloroprene Rubber (CR)
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.48 g/cc1.48 g/ccASTM D297, 15
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A >= 77>= 77ASTM D2240, Type A
 8282AVG; ASTM D2240, Type A
 87
@Treatment Temp. 100 °C,
Time 252000 sec
87
@Treatment Temp. 212 °F,
Time 70.0 hour
After Dry Heat Aging; ASTM D865
Tensile Strength at Break >= 13.05 MPa>= 1893 psiASTM D412 Method A
 16.18 MPa2347 psiAVG; ASTM D412 Method A
 16.18 MPa
@Treatment Temp. 100 °C,
Time 252000 sec
2347 psi
@Treatment Temp. 212 °F,
Time 70.0 hour
After Dry Heat Aging; ASTM D865
Tensile Stress at Strain  >= 2.36 MPa
@Strain 50 %
>= 343 psi
@Strain 50 %
Minimum; ASTM D412 Method A
 2.40 MPa
@Strain 25 %
348 psi
@Strain 25 %
Average; ASTM D412 Method A
 3.96 MPa
@Strain 50 %
574 psi
@Strain 50 %
Average; ASTM D412 Method A
 >= 5.34 MPa
@Strain 100 %
>= 774 psi
@Strain 100 %
Minimum; ASTM D412 Method A
 8.384 MPa
@Strain 100 %
1216 psi
@Strain 100 %
Average; ASTM D412 Method A
Elongation at Break >= 126 %>= 126 %ASTM D412 Method A
 182 %182 %AVG; ASTM D412 Method A
 182 %
@Treatment Temp. 100 °C,
Time 252000 sec
182 %
@Treatment Temp. 212 °F,
Time 70.0 hour
After Dry Heat Aging; ASTM D865
Modulus of Elasticity 0.01673 GPa2.426 ksiASTM D412 Method A
Poissons Ratio 0.500.50Calculated
Shear Modulus 0.00558 GPa0.809 ksiASTM D412 Method A
Secant Modulus 0.0157 GPa2.28 ksiASTM D412 Method A
Compression Set 29 %
@Temperature 100 °C,
Time 79200 sec
29 %
@Temperature 212 °F,
Time 22.0 hour
ASTM D395, Test B
 
Thermal PropertiesMetricEnglishComments
Glass Transition Temp, Tg -40.0 °C-40.0 °FASTM D1329
 
Descriptive Properties
Strain Energy / Unit Volume at 20% Elongation (psi)39

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Seals Eastern 5241 Neoprene / Chloroprene
Polychloroprene Rubber (CR)
Seals Eastern 7282 Neoprene / Chloroprene
Trelleborg Neoprene® C423 Chloroprene
Precision Polymer Engineering C40M Chloroprene Rubber

PSEAL50 / 80197

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.