MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

LyondellBasell GA675662 Petrothene® Linear Low Density Polyethylene  (discontinued **)
Categories: Polymer; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE); Linear Low Density Polyethylene (LLDPE), Rotational Molding Grade

Material Notes: PETROTHENE GA675662, a hexene LLDPE, pelletized rotational molding resin with excellent flow properties, can be used to produce a variety of objects such as toys, playground equipment, drums and agricultural and chemical storage containers. GA675662 exhibits good low temperature impact strength and warp resistance. It is UV-stabilized and available in a 35-mesh powder as MICROTHENE® MP675662.

Processing Techniques: Specific recommendations for conditions under which GA675662 should be processed can be made only when the end use and type of processing equipment are known.

Regulatory Status:GA675662 meets the requirements of Food and Drug Administration regulation, 21 CFR 177.1520. This regulation allows the use of this olefin polymer in "...articles or components of articles intended for use in contact with food." Specific limitations or conditions of use may apply. GA675662 is also being evaluated by the Underwriters Laboratories (UL) for flammability standard 94.

Information provided by manufacturer.

This product is from the former Equistar product line.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.939 g/cc0.0339 lb/in³Compression Molded; ASTM D1505
Melt Flow 5.2 g/10 min
@Load 2.16 kg,
Temperature 190 °C
5.2 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 20.5 MPa2970 psiCrosshead Speed - 2 in/min; Type IV Specimen (1/8 in); ASTM D638
Flexural Modulus, 1% Secant 869 MPa126000 psi1/8 in rotomolded sample; ASTM D790
Impact Test 63.7 J47.0 ft-lbat -40°F; 1/8 in rotomolded sample; ARM STD
 244 J180 ft-lbat -40°F; 1/4 in rotomolded sample; ARM STD
 
Compliance PropertiesMetricEnglishComments
FDA YesYesSee notes for details.

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for High Density Polyethylene (HDPE), Rotational Molding Grade
Trinseo EMERGE™ 9500CR Polycarbonate (PC) / Polyethylene Terephthalate (PET)
Overview of materials for Medium Density Polyethylene (MDPE), Rotational Molded
ExxonMobil Escorene® HD-8760 LHDPE Rotational Molding Grade
Bamberger Polymers Bapolene® 3039U Polyethylene, Rotational Molding Grade

PEQU0759 / 37228

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.