MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

LyondellBasell Hostacom Hostacom HYG 343L 356015 Polypropylene, Glass/Mineral Reinforced  (discontinued **)
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: Hostacom HYG 343L 356015 is a glass fiber reinforced PP homopolymer with very high melt flow rate. Product is UL listed. Applications: White Goods

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.25 g/cc0.0452 lb/in³ISO 1183-1A
Melt Flow 26 - 36 g/10 min
@Load 2.16 kg,
Temperature 230 °C
26 - 36 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 114 MPa16500 psiISO 527-1,-2
Elongation at Break 2.5 %2.5 %ISO 527-1,-2
Elongation at Yield 2.2 %2.2 %ISO 527-1,-2
Tensile Modulus 9.40 GPa1360 ksiISO 527-1,-2
Flexural Modulus 9.20 GPa1330 ksiTech.A; ISO 178/A1
Charpy Impact Unnotched  4.50 J/cm²
@Temperature 0.000 °C
21.4 ft-lb/in²
@Temperature 32.0 °F
ISO 179-1/1eU
 4.70 J/cm²
@Temperature 23.0 °C
22.4 ft-lb/in²
@Temperature 73.4 °F
ISO 179-1/1eU
Charpy Impact, Notched  0.800 J/cm²
@Temperature 0.000 °C
3.81 ft-lb/in²
@Temperature 32.0 °F
ISO 179-1/1eA
 0.850 J/cm²
@Temperature 23.0 °C
4.04 ft-lb/in²
@Temperature 73.4 °F
ISO 179-1/1eA
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 145 °C293 °FISO 75-1,-2
Vicat Softening Point 135 °C275 °FB50N; ISO 306
Flammability, UL94 HB
@Thickness 3.00 mm
HB
@Thickness 0.118 in
 
Descriptive Properties
Processing MethodInjection Molding

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LyondellBasell Hostacom HBC 181L 303612 Polypropylene, Mineral Reinforced
Trinseo Magnum™ 3416 SC Natural Plus ABS Resin
Celanese ZENITE 6330L LCP, 30% Mineral Reinforced
EMS-Grivory Grivory® GM-4H PA*-MD40
Borealis Daplen™ EE137AI Polypropylene Compound 10% Mineral Filled

PEQT7999 / 219635

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.