MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Elektro-Isola G-Etronax EP 22 Epoxy, Glass Fabric Reinforcement, Light Yellow, Tubes
Categories: Polymer; Thermoset; Epoxy

Material Notes: Description: Particularly good electrical and mechanical properties. Extremely high mechanical strength, even at high temperatures. Retains electrical properties at high air humidity. High resistance to chemicals.

Applications: Engineering and insulation material in large rotating electrical machines and insulation cylinders in dry transformers.

Information provided by Elektro-Isola

Key Words: IEC/EN 61212-3-1 EP GC 22, DIN 7735 Hgw 2375.4, NEMA LI G-11
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.75 g/cc
@Thickness >=0.000 mm
0.0632 lb/in³
@Thickness >=0.000 in
24hr/23°C/50% RH; ISO 1183-A; IEC/EN 61212-2 7.3
Water Absorption 0.020 %0.020 %24hr/50°C+24hr in water at 23°C; ISO 62-1; IEC/EN 61212-2 7.2
 
Mechanical PropertiesMetricEnglishComments
Flexural Strength 350 MPa
@Diameter >=100 mm
50800 psi
@Diameter >=3.94 in
24hr/23°C/50% RH, 230 Mpa measured at 150°C; ISO 178; IEC/EN 61212-2 5.1
Compressive Strength 200 MPa
@Temperature 23.0 °C,
Time 86400 sec
29000 psi
@Temperature 73.4 °F,
Time 24.0 hour
50% RH, Axial; ISO 604; IEC/EN 61212-2 5.2
Adhesive Bond Strength 400 MPa
@Diameter <=100 mm
58000 psi
@Diameter <=3.94 in
24hr/23°C/50% RH; IEC 60212-2; IEC/EN 61212-2 5.3
 
Electrical PropertiesMetricEnglishComments
Insulation Resistance 1.00e+10 ohm
@Diameter 8.00 - 10.0 mm
1.00e+10 ohm
@Diameter 0.315 - 0.394 in
24hr/50°C+24h in water at 23°C; IEC; IEC/EN 61212-2 6.2
Dielectric Constant  4.5
@Frequency 50 Hz
4.5
@Frequency 50 Hz
96hr/105°C+1hr/23°C/20%RH; IEC 250; IEC/EN 61212-2 6.3
 4.5
@Frequency 1e+6 Hz
4.5
@Frequency 1e+6 Hz
96hr/105°C+1hr/23°C/20%RH; IEC 250; IEC/EN 61212-2 6.3
Dielectric Strength 11.0 kV/mm
@Thickness 3.00 mm
279 kV/in
@Thickness 0.118 in
24hr/23°C/50% RH+1hr/oil 90°C; Perpendicular; IEC 60243-1; IEC/EN 61212-2 6.1.2.1
 2.40 kV/mm
@Diameter >=3.00 mm
61.0 kV/in
@Diameter >=0.118 in
24hr/23°C/50% RH+1hr/oil 90°C; Parallel; IEC 60243-1; IEC/EN 61212-2 6.1.2.1
Dissipation Factor  0.010
@Frequency 50 Hz
0.010
@Frequency 50 Hz
96hr/105°C+1hr/23°C/20%RH; IEC 250; IEC/EN 61212-2 6.3
 0.010
@Frequency 1000 Hz
0.010
@Frequency 1000 Hz
96hr/105°C+1hr/23°C/20%RH; IEC 250; IEC/EN 61212-2 6.3
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Inert 160 °C
@Thickness 3.00 mm,
Time 7.20e+7 sec
320 °F
@Thickness 0.118 in,
Time 20000 hour
IEC 60695-11-10; IEC/EN 61212-2 7.1

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Elektro-Isola G-Etronax EP 10 Epoxy, Glass Fabric Reinforcement, Light Yellow, Tubes
Elektro-Isola Etronax MF Phenolic, Cotton Fabric Reinforcement, Brown, Tubes
Elektro-Isola Etronax MMMF Phenolic, Cotton Fabric Reinforcement, Brown, Tubes
Elektro-Isola G-Etronax EP 11 Epoxy, Glass Fabric Reinforcement, Green, Tubes
Elektro-Isola Etronax MMF Phenolic, Cotton Fabric Reinforcement, Brown, Tubes

PELEKT014 / 126890

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.