MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Lucite International Elvacite® 4409 Acrylic Resin, Hydroxyl Functional
Categories: Polymer; Thermoplastic; Acrylic (PMMA)

Material Notes: Elvacite® 4409 is a solid methacrylate copolymer bead resin designed for use in formulating environmentally sound thermosetting coatings and adhesives. The resin may be used as the main binder in acrylic systems, or blended with other resins to improve weather resistance and clarity. Elvacite® 4409 is solvent free to provide maximum formulation latitude.

Information provided by Lucite International

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Viscosity Measurement 0.180.18Inherent viscosity, 0.25 g polymer in 50 ml of methylene chloride; No. 50 Cannon-Fenske viscometer.
Molecular Weight 31000 g/mol31000 g/mol
 
Chemical PropertiesMetricEnglishComments
Total Acid Number 0.000.00
 
Thermal PropertiesMetricEnglishComments
Glass Transition Temp, Tg 104 °C219 °F
 
Descriptive Properties
Hydroxyl Number4

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Lucite International Elvacite® 4400 Acrylic Resin
Lucite International Elvacite® 4402 Acrylic Resin
Lucite International Elvacite® 2044 Acrylic Resin
Lucite International Elvacite® 2021E Acrylic Resin

PLUCIT9486 / 150200

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.