MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

BNZ Materials Transite HT Low Temperature Industrial Board
Categories: Ceramic; Oxide

Material Notes: These non-asbestos, monolithic fiber cement industrial boards are used in environments up to 1000°F where high strength is the primary concern. These fiber cement boards are used in the foundry industry for flask liners, core, drying and carry plates, and induction furnace casings. Electrical applications include busbar supports, aluminum pot insulation, and electrode arm insulators.

Information provided by BNZ Materials Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.60 g/cc0.0579 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Modulus of Rupture 0.0190 GPa2.76 ksi
Compressive Yield Strength 44.8 MPa
@Strain 5.0 %
6500 psi
@Strain 5.0 %
Compressive Strength 71.7 MPa10400 psiultimate load
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 7.10e+10 ohm-cm7.10e+10 ohm-cmASTM D257
Dielectric Strength 1.38 kV/mm35.0 kV/inASTM D495
Arc Resistance 260 sec260 secASTM D495
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 0.340 W/m-K
@Temperature 121 °C
2.36 BTU-in/hr-ft²-°F
@Temperature 250 °F
Shrinkage  0.85 %
@Temperature 316 °C,
Time 86400 sec
0.85 %
@Temperature 600 °F,
Time 24.0 hour
Length/width
 3.7 %
@Temperature 316 °C,
Time 86400 sec
3.7 %
@Temperature 600 °F,
Time 24.0 hour
Thickness
 
Component Elements PropertiesMetricEnglishComments
H2O, Water 12 %12 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BNZ Materials Transite 1000 Low Temperature Industrial Board
Morgan Advanced Ceramics Kaowool® Cement B
Morgan Advanced Ceramics Firemaster Board 550 Thermal Ceramic
Pyrotek ISOMAG® 45 Thermal Insulation Board
Wacker Silres® BS Powder A Silicone Masonry Water Repellent

CBNZ932 / 149172

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.