MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

INEOS Styrolution Novodur® P2M-AT ABS
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS), Impact Grade, Molded

Material Notes: Novodur® P2M-AT is a medium impact, high gloss injection molding grade with good flowability and contains an antistatic additive. medium impact, high gloss.

Applications: household appliances, telecommunication.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.04 g/cc0.0376 lb/in³ISO 1183
Linear Mold Shrinkage 0.0040 - 0.0070 cm/cm0.0040 - 0.0070 in/inISO 294-4
Linear Mold Shrinkage, Flow 0.0040 - 0.0070 cm/cm0.0040 - 0.0070 in/inTest Condition: 60x60x2; ISO 294-4
Linear Mold Shrinkage, Transverse 0.0040 - 0.0070 cm/cm0.0040 - 0.0070 in/inTest Condition: 60x60x2; ISO 294-4
Melt Flow 22 g/10 min
@Load 10.0 kg,
Temperature 220 °C
22 g/10 min
@Load 22.0 lb,
Temperature 428 °F
Volumetric; cm3/10 min; ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Ball Indentation Hardness 95.0 MPa13800 psiISO 2039-1
Tensile Strength, Yield 39.0 MPa5660 psiISO 527
Elongation at Break >= 15 %>= 15 %ISO 527
Elongation at Yield 2.1 %2.1 %ISO 527
Tensile Modulus 2.30 GPa334 ksiISO 527
Flexural Strength 60.0 MPa8700 psiISO 178
Flexural Modulus 2.10 GPa305 ksiISO 178
Izod Impact, Notched (ISO)  11.0 kJ/m²
@Temperature -30.0 °C
5.23 ft-lb/in²
@Temperature -22.0 °F
ISO 180/A
 23.0 kJ/m²
@Temperature 23.0 °C
10.9 ft-lb/in²
@Temperature 73.4 °F
ISO 180/A
Charpy Impact Unnotched  12.0 J/cm²
@Temperature -30.0 °C
57.1 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eU
 18.0 J/cm²
@Temperature 23.0 °C
85.7 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched  1.10 J/cm²
@Temperature -30.0 °C
5.23 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eA
 2.20 J/cm²
@Temperature 23.0 °C
10.5 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant  3.0
@Frequency 1e+6 Hz
3.0
@Frequency 1e+6 Hz
IEC 60250
 3.1
@Frequency 100 Hz
3.1
@Frequency 100 Hz
IEC 60250
Dissipation Factor  0.0060
@Frequency 100 Hz
0.0060
@Frequency 100 Hz
IEC 60250
 0.0080
@Frequency 1e+6 Hz
0.0080
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 600 V600 VIEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear 100 µm/m-°C55.6 µin/in-°FISO 11359
Deflection Temperature at 0.46 MPa (66 psi) 97.0 °C207 °Fannealed 4 hours at 80°C; ISO 75
Deflection Temperature at 1.8 MPa (264 psi) 93.0 °C199 °Fannealed 4 hours at 80°C; ISO 75
Vicat Softening Point 98.0 °C
@Load 5.10 kg
208 °F
@Load 11.2 lb
VST/B/50. 50C/h; ISO 306
 
Processing PropertiesMetricEnglishComments
Melt Temperature 230 - 260 °C446 - 500 °FISO 294
Mold Temperature 60.0 - 80.0 °C140 - 176 °FISO 294
Injection Velocity 240 mm/sec9.45 in/secISO 294
Drying Temperature 80.0 °C
@Time 7200 - 14400 sec
176 °F
@Time 2.00 - 4.00 hour

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
INEOS Styrolution Novodur® P2M-V ABS Pellets
Ineos ABS Lustran® H802
Ineos ABS NOVODUR® P2T ABS, Injection Grade
Ineos ABS NOVODUR® P3T ABS, Injection Grade
Ineos ABS Lustran® H801

PINEA901 / 107172

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.