MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Carlson 90 10 Cu Ni Copper-Nickel Alloy
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: General Description

Carlson Alloy 90 10 Cu Ni is a copper-based alloy developed as a cost-effective substitute for 70 30 Cu Ni. An addition of approximately 1.4% iron was made to increase its resistance to general corrosion, erosion and impingement corrosion resulting form the turbulent flow of water containing air bubbles and silt flowing at a high velocity. 90 10 Cu Ni has good strength at moderately elevated temperatures. It can be fabricated by both hot and cold-working procedures, and is readily weldable.

90 10 Cu Ni has excellent resistance to corrosion by fresh water, brackish water, and sea water. It is not recommended for usage in heavily polluted water containing sewage and industrial wastes. 90 10 Cu Ni resists attack by phosphoric, sulfuric, and mild organic acids. It is attacked by chromic, hydrochloric and nitric acids. 90 10 Cu Ni is also resistant to the alkali chlorides, nitrates, sulfates and to ammonia and ammonium compounds.

Applications

90 10 Cu Ni is widely used in marine service, offshore platform sea water piping, tidewater power plants, desalination plants, oil refineries, and in the chemical process industry.

Product applications include condenser tubes and plates, distiller tubes, tube sheets and baffles for condensers and heat exchangers, evaporator and heat exchanger tubes, salt water piping, water boxes, ship hulls and hot water tanks.

Information provided by Carlson

Key Words: UNS C70600
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.94 g/cc0.323 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break >= 276 MPa>= 40000 psi
Tensile Strength, Yield >= 103 MPa
@Strain 0.2 %
>= 15000 psi
@Strain 0.2 %
Elongation at Break >= 30 %>= 30 %
Modulus of Elasticity 124 GPa18000 ksi
 
Thermal PropertiesMetricEnglishComments
CTE, linear 17.1 µm/m-°C
@Temperature 20.0 - 300 °C
9.50 µin/in-°F
@Temperature 68.0 - 572 °F
Specific Heat Capacity 0.377 J/g-°C
@Temperature 20.0 °C
0.0900 BTU/lb-°F
@Temperature 68.0 °F
 
Component Elements PropertiesMetricEnglishComments
Carbon, C <= 0.050 %<= 0.050 %
Copper, Cu 85.59 - 90 %85.59 - 90 %
Iron, Fe 1.0 - 1.8 %1.0 - 1.8 %
Lead, Pb <= 0.020 %<= 0.020 %
Manganese, Mn <= 1.0 %<= 1.0 %
Nickel, Ni 9.0 - 11 %9.0 - 11 %
Phosphorus, P <= 0.020 %<= 0.020 %
Sulfur, S <= 0.020 %<= 0.020 %
Zinc, Zn <= 0.50 %<= 0.50 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Copper nickel 10%, UNS C70600
Carlson 70 30 Cu Ni Copper-Nickel Alloy
Sandvik Osprey 90/10 Cu Sn Powder (Grade 95% - 16)
Sandvik Osprey 90/10 Cu Sn Powder (Grade 90% - 22)
Murtfeldt Murflor® + Bronze Polytetrafluoroethylene, 60% Bronze

NCARLSO27 / 15834

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.