MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Phillips 66 X/C® 5606H ISO Grade 15 Aviation Hydraulic Fluid
Categories: Fluid; Lubricant

Material Notes: Phillips 66®X/C 5606H and X/C 5606A Aviation Hydraulic Fluids are mineral oil-based, high viscosity index, ashless (zinc-free) antiwear hydraulic fluids designed to meet the severe demands of aerospace and industrial applications. They have excellent oxidation resistance and outstanding low-temperature properties for use over a wide temperature range. They provide excellent wear protection for hydraulic pumps and motors, protect hydraulic system components against rust and corrosion, and are resistant to excessive foam buildup that can cause poor or sluggish hydraulic system response. X/C 5606H Aviation Hydraulic Fluid meets the cleanliness requirements for “super clean” hydraulic fluid for use in modern aircraft hydraulic systems. X/C 5606A Aviation Hydraulic Fluid is recommended for use in hydraulic systems that do not require a “super clean” fluid. Both fluids are dyed red for identification and leak detection purposes.

Applications: X/C Aviation Hydraulic Fluids are recommended for use in non-pressurized systems operating between -54°C and 90°C (-65°F to 194°F), and in pressurized systems operating between -54°C and 135°C (-65°F to 275°F) at pressures up to 3,000 psi. Typical applications include:

  • Aircraft and missile control systems, autopilots and shock absorbers
  • Auto wreckers, boom trucks and electrical service equipment (cherry pickers) where all-weather performance is required
  • Industrial robotics
  • Hydraulic systems that require a “super clean” fluid for extended service life and reliability (X/C 5606H)
X/C 5606H Aviation Hydraulic Fluid meets the requirements of:
  • U.S. Military Specification MIL-PRF-5606H (supercedes MIL-O-5606, AN-O-336, AN-VV-O-336 and AAF-3580)
X/C 5606A Aviation Hydraulic Fluid meets the requirements of:
  • U.S. Military Specification MIL-H-5606A (obsolete)
Features/Benefits:
  • Very high viscosity index for use over a wide temperature range
  • Outstanding low-temperature properties
  • Excellent wear protection
  • Resists deposit formation and viscosity increase due to oxidation
  • Protects against rust and corrosion
  • Good foam resistance
  • Does not contain zinc or other heavy metals

Information provided by Phillips 66 Lubricants.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.871 g/cc0.871 g/cc
Density 0.869 g/cc0.0314 lb/in³
API Gravity 31 °31 °
Particle Size 5.0 - 15 µm5.0 - 15 µmParticle Contamination: 1200; FTM 3012
 16 - 25 µm16 - 25 µmParticle Contamination: 175
 26 - 50 µm26 - 50 µmParticle Contamination: 60
 51 - 100 µm51 - 100 µmParticle Contamination: 5
 >= 100 µm>= 100 µmParticle Contamination: 0
Viscosity  495 cP
@Temperature -40.0 °C
495 cP
@Temperature -40.0 °F
Kinematic
 2450 cP
@Temperature -54.0 °C
2450 cP
@Temperature -65.2 °F
Kinematic
Viscosity Measurement 382382Index
Kinematic Viscosity at 40°C (104°F) 13.5 cSt13.5 cSt
Kinematic Viscosity at 100°C (212°F) 5.1 cSt5.1 cSt
Evaporation Loss 13.6 %
@Temperature 71.0 °C,
Time 259000 sec
13.6 %
@Temperature 160 °F,
Time 72.0 hour
ASTM D972
 
Chemical PropertiesMetricEnglishComments
Total Acid Number 0.0500.050[mg KOH/g]; ASTM D974
 
Mechanical PropertiesMetricEnglishComments
Four Ball Wear 0.650 mm0.0256 inScar Diameter; ASMT D4172
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength 49.6 kV/mm1260 kV/inno thickness given; ASTM D877
 
Thermal PropertiesMetricEnglishComments
Pour Point -64.0 °C-83.2 °F
Flash Point 90.0 °C194 °FPMCC
 
Descriptive Properties
ColorRed
Composition60 ppmWater, ASTM D6304
Copper Corrosion1b71°C (160°F), 72 hours, ASTM D130
Gravimetric Filtration6 minutesFTM 313, mg/100 ml, 0.45 microns @ 25°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ExxonMobil Mobil Aero HF
Phillips 66 X/C® 5606A ISO Grade 15 Aviation Hydraulic Fluid
ChevronTexaco ISO 22 Hydraulic Oil AW
ChevronTexaco ISO 10 Hydraulic Oil AW

WCON6372 / 210095

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.