Inno-Comp INNOPOL® CS 2-9000 MA B Polypropylene Copolymer
Categories:
Polymer
;
Thermoplastic
;
Polypropylene (PP)
;
Polypropylene Copolymer
Material Notes:
INNOPOL® CS 2-9000 MA B is a black colored, high melt flow copolymer with antistatic additive.
INNOPOL® CS 2-9000 MA B is developed for producing injection molded automotive components.
All information provided by INNO-COMP.
Key Words:
PP
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Density
0.900
g/cc
@Temperature 23.0 °C
0.0325
lb/in³
@Temperature 73.4 °F
ISO 1183
Linear Mold Shrinkage, Flow
0.014
cm/cm
0.014
in/in
ISO 294
Linear Mold Shrinkage, Transverse
0.022
cm/cm
0.022
in/in
ISO 294
Melt Flow
36
g/10 min
@Load 2.16 kg,
Temperature 230 °C
36
g/10 min
@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Mechanical Properties
Metric
English
Comments
Tensile Strength, Yield
27.0
MPa
3920
psi
50 mm/min; ISO 527-1,-2
Elongation at Break
25 %
25 %
ISO 527-1,-2
Elongation at Yield
4.5 %
4.5 %
50 mm/min; ISO 527-1,-2
Tensile Modulus
1.405
GPa
203.8
ksi
1 mm/min; ISO 527-1,-2
Flexural Modulus
1.55
GPa
225
ksi
2 mm/min; ISO 178
Charpy Impact Unnotched
89.0
J/cm²
@Temperature -30.0 °C
424
ft-lb/in²
@Temperature -22.0 °F
Partial Break; ISO 179/1eU
NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched
0.450
J/cm²
@Temperature -30.0 °C
2.14
ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eA
1.00
J/cm²
@Temperature 23.0 °C
4.76
ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
Thermal Properties
Metric
English
Comments
Melting Point
163
°C
325
°F
DSC; ISO 11357-1,-3
Deflection Temperature at 0.46 MPa (66 psi)
108
°C
226
°F
ISO 75-1,-2
Deflection Temperature at 1.8 MPa (264 psi)
57.0
°C
135
°F
ISO 75-1,-2
Vicat Softening Point
79.0
°C
174
°F
B120; ISO 306
148
°C
298
°F
A120; ISO 306
Flammability, UL94
HB
@Thickness 1.60 mm
HB
@Thickness 0.0630 in
FMVSS 302
Descriptive Properties
Automotive Materials
Pass
FMVSS 302
Color
Black
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
ExxonMobil AP03B Polypropylene Impact Copolymer
Reliance Industries Repol B120MA Polypropylene
Reliance Industries Repol B220MN Polypropylene
Inno-Comp INNOPOL® CS 2-9000 MA N Polypropylene Copolymer
Formosa Plastics Formolene® 6335N Impact Copolymer Polypropylene
PINNO051 / 82712
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.