MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Rhenium, Re; Annealed
Categories: Metal; Nonferrous Metal; Refractory Metal; Pure Element

Material Notes: Annealed applies only to tensile and/or hardness values; other property values are typical of the element. Stress relieving temperature 900-1200°C. Recrystallization temperature, 1 hour, is 1400-1600°C.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 21.03 g/cc0.7598 lb/in³
Vapor Pressure  1.00e-14 bar
@Temperature 1525 °C
7.50e-12 torr
@Temperature 2777 °F
 4.00e-11 bar
@Temperature 2000 °C
3.00e-8 torr
@Temperature 3630 °F
 1.10e-9 bar
@Temperature 2200 °C
8.25e-7 torr
@Temperature 3990 °F
 1.90e-8 bar
@Temperature 2400 °C
0.0000143 torr
@Temperature 4350 °F
 1.60e-7 bar
@Temperature 2600 °C
0.000120 torr
@Temperature 4710 °F
 0.00000170 bar
@Temperature 2800 °C
0.00128 torr
@Temperature 5070 °F
 0.0000110 bar
@Temperature 3000 °C
0.00825 torr
@Temperature 5430 °F
 
Chemical PropertiesMetricEnglishComments
Atomic Mass 186.207186.2071995
Atomic Number 7575
Thermal Neutron Cross Section 86 barns/atom86 barns/atom
X-ray Absorption Edge 0.17311 Å0.17311 ÅK
 0.99009 Å0.99009 ÅLI
 1.03645 Å1.03645 ÅLII
 1.1772 Å1.1772 ÅLIII
Electronegativity 1.91.9Pauling
Ionic Radius 0.560 Å0.560 ÅCrystal Ionic Radius for Valence +7
 0.720 Å0.720 ÅCrystal Ionic Radius for Valence +4
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 165165Converted from Vickers for 3000 kg load/10 mm ball Brinell test.
Hardness, Rockwell A 5252Converted from Vickers.
Hardness, Rockwell B 8585Converted from Vickers.
Hardness, Vickers 170170
Tensile Strength, Ultimate 1070 MPa155000 psi
 410 MPa
@Temperature 1200 °C
59500 psi
@Temperature 2190 °F
 620 MPa
@Temperature 800 °C
89900 psi
@Temperature 1470 °F
Tensile Strength, Yield 290 MPa42100 psi
Elongation at Break 15 - 25 %15 - 25 %
Modulus of Elasticity 469 GPa68000 ksi
Poissons Ratio 0.2960.296
Shear Modulus 176 GPa25500 ksi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity  0.0000193 ohm-cm
@Temperature 20.0 °C
0.0000193 ohm-cm
@Temperature 68.0 °F
 0.0000254 ohm-cm
@Temperature 100 °C
0.0000254 ohm-cm
@Temperature 212 °F
 0.0000400 ohm-cm
@Temperature 300 °C
0.0000400 ohm-cm
@Temperature 572 °F
 0.0000526 ohm-cm
@Temperature 500 °C
0.0000526 ohm-cm
@Temperature 932 °F
 0.0000630 ohm-cm
@Temperature 700 °C
0.0000630 ohm-cm
@Temperature 1290 °F
 0.0000725 ohm-cm
@Temperature 900 °C
0.0000725 ohm-cm
@Temperature 1650 °F
 0.0000805 ohm-cm
@Temperature 1100 °C
0.0000805 ohm-cm
@Temperature 2010 °F
 0.0000870 ohm-cm
@Temperature 1300 °C
0.0000870 ohm-cm
@Temperature 2370 °F
 0.0000930 ohm-cm
@Temperature 1500 °C
0.0000930 ohm-cm
@Temperature 2730 °F
 0.0000985 ohm-cm
@Temperature 1700 °C
0.0000985 ohm-cm
@Temperature 3090 °F
 0.000103 ohm-cm
@Temperature 1900 °C
0.000103 ohm-cm
@Temperature 3450 °F
 0.0001065 ohm-cm
@Temperature 2100 °C
0.0001065 ohm-cm
@Temperature 3810 °F
 0.000109 ohm-cm
@Temperature 2300 °C
0.000109 ohm-cm
@Temperature 4170 °F
Magnetic Susceptibility 3.63e-73.63e-7cgs/g
Critical Magnetic Field Strength, Oersted 195 - 205195 - 205
Critical Superconducting Temperature 1.691 - 1.703 K1.691 - 1.703 K2.3 K max for Re II
 
Thermal PropertiesMetricEnglishComments
Heat of Fusion 178 J/g76.6 BTU/lb
CTE, linear  6.12 µm/m-°C
@Temperature 500 °C
3.40 µin/in-°F
@Temperature 932 °F
 6.20 µm/m-°C
@Temperature 20.0 °C
3.44 µin/in-°F
@Temperature 68.0 °F
 6.20 µm/m-°C
@Temperature 250 °C
3.44 µin/in-°F
@Temperature 482 °F
 6.65 µm/m-°C
@Temperature 1000 °C
3.69 µin/in-°F
@Temperature 1830 °F
Specific Heat Capacity  0.134 J/g-°C
@Temperature 500 °C
0.0320 BTU/lb-°F
@Temperature 932 °F
 0.138 J/g-°C
@Temperature 25.0 °C
0.0330 BTU/lb-°F
@Temperature 77.0 °F
 0.150 J/g-°C
@Temperature 1000 °C
0.0359 BTU/lb-°F
@Temperature 1830 °F
 0.161 J/g-°C
@Temperature 1000 °C
0.0385 BTU/lb-°F
@Temperature 1830 °F
 0.177 J/g-°C
@Temperature 1500 °C
0.0423 BTU/lb-°F
@Temperature 2730 °F
 0.199 J/g-°C
@Temperature 2000 °C
0.0476 BTU/lb-°F
@Temperature 3630 °F
Thermal Conductivity 39.6 W/m-K275 BTU-in/hr-ft²-°F
Melting Point 3180 °C5760 °F
Boiling Point 5596 °C10100 °F
Maximum Service Temperature, Inert 2380 °C4320 °Fvaporization<1% after 10 hours
 
Optical PropertiesMetricEnglishComments
Emissivity (0-1) 0.42
@Temperature 0.000 - 2000 °C,
Wavelength 655 nm
0.42
@Temperature 32.0 - 3630 °F,
Wavelength 655 nm
 
Component Elements PropertiesMetricEnglishComments
Rhenium, Re 100 %100 %
 
Descriptive Properties
CAS Number7440-15-5

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Rhenium, Re; Deformed
Rhodium, Rh; Annealed
Vanadium, V; Cold Rolled
Chromium, Cr; As-Swaged
Tantalum, Ta; Annealed

AMERe00 / 91

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.