MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Lotte Advanced Materials Starex® VE-0860 P ABS  (discontinued **)
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS), Unreinforced, Flame Retardant

Material Notes: Flame Retardant, Home Appliances

Information provided by Lotte Advanced Materials

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.18 g/cc1.18 g/ccNatural or representative color; ASTM D792
Linear Mold Shrinkage, Flow 0.0042 - 0.0052 cm/cm
@Thickness 3.20 mm
0.0042 - 0.0052 in/in
@Thickness 0.126 in
ASTM D955
Linear Mold Shrinkage, Transverse 0.0045 - 0.0055 cm/cm
@Thickness 3.20 mm
0.0045 - 0.0055 in/in
@Thickness 0.126 in
ASTM D955
Melt Flow 14 g/10 min
@Load 10.0 kg,
Temperature 220 °C
14 g/10 min
@Load 22.0 lb,
Temperature 428 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 102102ASTM D785
Tensile Strength at Break 21.6 MPa3130 psi5 mm/min; ASTM D638
Tensile Strength, Yield 37.3 MPa5400 psi5 mm/min; ASTM D638
Elongation at Break 9.0 %9.0 %5 mm/min; ASTM D638
Tensile Modulus 1.54 GPa223 ksi5 mm/min; ASTM D638
Flexural Strength 54.9 MPa7960 psi2.8 mm/min; ASTM D790
Flexural Modulus 1.96 GPa284 ksi2.8 mm/min; ASTM D790
Izod Impact, Notched  1.37 J/cm
@Thickness 6.35 mm
2.57 ft-lb/in
@Thickness 0.250 in
ASTM D256
 1.47 J/cm
@Thickness 3.17 mm
2.76 ft-lb/in
@Thickness 0.125 in
ASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 89.0 °C
@Thickness 6.40 mm
192 °F
@Thickness 0.252 in
ASTM D648
Vicat Softening Point 99.0 °C210 °FB/50; ISO R 306
Flammability, UL94  V-2
@Thickness 1.50 mm
V-2
@Thickness 0.0591 in
 V-2
@Thickness 2.50 - 2.70 mm
V-2
@Thickness 0.0984 - 0.106 in
 V-0
@Thickness 2.00 mm
V-0
@Thickness 0.0787 in
 5VB
@Thickness 2.50 - 2.70 mm
5VB
@Thickness 0.0984 - 0.106 in
 
Optical PropertiesMetricEnglishComments
Yellow Index 15 %
@Thickness 3.20 mm
15 %
@Thickness 0.126 in
ASTM D1925

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Lotte Advanced Materials Starex® VE-0856 (VE-0856U UV) Flame Retardant Grade ABS
Lotte Advanced Materials Starex® VE-0855YS ABS, Unreinforced FR
LG Chemical AF360S ABS, TBBA-free Flame Retardant, Low Flow
LG Chemical AF305HT ABS, Flame Retardant, Heat Resistance
Chi Mei Polylac® PA-765B ABS - Flame Retardant

PLOTT9931 / 205794

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.