MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Pure Lead (Corroding Lead), UNS L50042, Chill Cast
Categories: Metal; Nonferrous Metal; Lead Alloy; Pure Element

Material Notes: 99.94% min. Pb is a typical specification for pure lead. This grade is the most common in the US and is used as raw material for lead chemicals and pigments.

Key Words: Lead Alloys, ASTM B29 (Corroding Lead); B749
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 11.36 g/cc0.4104 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 3.2 - 4.53.2 - 4.510 mm ball/100 kg load, 10 sec.
Tensile Strength, Ultimate 14.0 MPa2030 psi
Elongation at Break 47 %47 %in 50 mm
Modulus of Elasticity 14.0 GPa2030 ksi
Fatigue Strength 3.00 MPa
@# of Cycles 1.00e+7
435 psi
@# of Cycles 1.00e+7
Typical; heat treatment unknown
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000210 ohm-cm0.0000210 ohm-cm
Magnetic Susceptibility -1.20e-7-1.20e-7cgs/g
Critical Magnetic Field Strength, Oersted 802 - 804802 - 804
Critical Superconducting Temperature 7.19 - 7.202 K7.19 - 7.202 K
 
Thermal PropertiesMetricEnglishComments
Heat of Fusion 24.0 J/g10.3 BTU/lb
CTE, linear 29.3 µm/m-°C
@Temperature 17.0 - 100 °C
16.3 µin/in-°F
@Temperature 62.6 - 212 °F
Specific Heat Capacity 0.129 J/g-°C0.0308 BTU/lb-°F
Thermal Conductivity 35.0 W/m-K243 BTU-in/hr-ft²-°F
Melting Point 328 °C622 °F
Boiling Point 1749 °C3180 °F
 
Optical PropertiesMetricEnglishComments
Emissivity (0-1) 0.630.63
Reflection Coefficient, Visible (0-1) 0.620.62589 nm
 
Component Elements PropertiesMetricEnglishComments
As + Sb + Sn <= 0.0020 %<= 0.0020 %
Bismuth, Bi <= 0.050 %<= 0.050 %
Copper, Cu <= 0.0040 %<= 0.0040 %Includes silver
Iron, Fe <= 0.0020 %<= 0.0020 %
Lead, Pb >= 99.94 %>= 99.94 %
Silver, Ag <= 0.0015 %<= 0.0015 %
Zinc, Zn <= 0.0010 %<= 0.0010 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Battery Grid Alloy, Lead-Calcium-Tin (UNS L50740)
Pure Lead (Corroding Lead), UNS L50042, Sand Cast
Battery Grid Alloy (Pb-Ca-Sn), UNS L50780
Hard Lead (94Pb-6Sb), UNS L53105, Chill Cast
Copperized Soft Lead, UNS L51125

MLPb03 / 12213

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.