MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Dow TUFLIN™ HS-7028 NT 7 Linear Low Density Polyethylene Resin
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE)

Material Notes:
  • Hexene Linear Low Density Resin
  • General Purpose Resin
  • Excellent Strength
  • Complies with U.S. FDA 21 CFR 177.1520 (c) 3.1a (with Restrictions)
TUFLIN™ HS-7028 NT 7 is an ethylene-hexene copolymer, designed for good strength and processability. This product is recommended for general-purpose packaging applications from thick gauge, heavy duty bags to high speed thin gauge applications.

Information provided by Dow

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.918 g/cc0.0332 lb/in³ASTM D792
Thickness 20.3 microns0.800 mil
Melt Flow 1.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
1.0 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Film Tensile Strength at Yield, MD 15.98 MPa2318 psiASTM D882
Film Tensile Strength at Yield, TD 15.42 MPa2237 psiASTM D882
Film Elongation at Break, MD 577 %577 %ASTM D882
Film Elongation at Break, TD 800 %800 %ASTM D882
Secant Modulus, MD 0.20403 GPa29.592 ksi2% Secant; ASTM D882
Secant Modulus, TD 0.2332 GPa33.83 ksi2% Secant; ASTM D882
Impact 9.09.0[lbf]; Puncture Resistance Force; Dow Method
 253253[ft-lbf/in3]; Puncture Resistance; Dow Method
 35643564[ft-lbf/in3]; Toughness MD; ASTM D882
 41184118[ft-lbf/in3]; Toughness TD; ASTM D882
Puncture Energy 3.39 J2.50 ft-lbDow Method
Elmendorf Tear Strength MD 296 g296 gMethod B; ASTM D1922
Elmendorf Tear Strength TD 674 g674 gMethod B; ASTM D1922
Elmendorf Tear Strength, MD 14.6 g/micron370 g/milASTM D1922
Elmendorf Tear Strength, TD 33.17 g/micron842.5 g/milASTM D1922
Dart Drop Test 94.0 g0.207 lbMethod A; ASTM D1709
 <= 100 g<= 0.221 lbMethod B; ASTM D1709
Film Tensile Strength at Break, MD 60.68 MPa8801 psiASTM D882
Film Tensile Strength at Break, TD 48.17 MPa6987 psiASTM D882
Heat Seal Strength, Ultimate 9.80 N2.20 lb (f)at 150°C, 0.5 sec dwell, 40 psi bar pressure, pull speed 10 (in./min.); Dow Method
Heat Seal Strength Initiation Temperature 110 °C230 °F1 lb/in heat seal strength; 0.5 sec dwell, 40 psi bar pressure, pull speed 10 (in./min.); Dow Method
 
Thermal PropertiesMetricEnglishComments
Melting Point 124 °C255 °FDow Method (DSC)
Vicat Softening Point 103 °C217 °FASTM D1525
 
Optical PropertiesMetricEnglishComments
Haze 12 %12 %ASTM D1003
Gloss 50 %50 %45°; ASTM D2457
 62 %62 %20°; ASTM D2457
 
Compliance PropertiesMetricEnglishComments
FDA YesYesSee notes for details.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Dow TUFLIN™ HS-7021 NT 7 Linear Low Density Polyethylene Resin
Dow LDPE 641I Low Density Polyethylene, Liner Film Grade
Dow TUFLIN™ HS-7041 NT 7 Linear Low Density Polyethylene Resin
Dow TUFLIN™ HS-7065 NT 7 Linear Low Density Polyethylene Resin
Dow TUFLIN™ HS-7066 NT 7 Linear Low Density Polyethylene Resin

PDOW1440 / 30658

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.