MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Mocom (ALBIS) ALTECH® ASA A 1000/128 UV ASA
Categories: Polymer; Thermoplastic; ASA Polymer; Acrylonitrile/Styrene/Acrylate (ASA), 15% Glass Reinforced

Material Notes: Base Polymer: Acrylonitile/Sytrene/Acrylate/Coplymer

Filler/Additive System: Light Stabilizer

Special Features: Good chemical resistance, high heat stabilized, injection molding grade, UV stabilized, good weathering resistance

Typical Application: Various

Information provided by Albis Plastics

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.11 g/cc0.0401 lb/in³ISO 1183
Linear Mold Shrinkage 0.0040 - 0.0080 cm/cm
@Time 86400 sec
0.0040 - 0.0080 in/in
@Time 24.0 hour
ISO 294-4
Melt Flow 6.0 g/10 min
@Load 10.0 kg,
Temperature 220 °C
6.0 g/10 min
@Load 22.0 lb,
Temperature 428 °F
ISO 1133
Storage Temperature <= 30.0 °C<= 86.0 °Fdry, protected from light
 
Mechanical PropertiesMetricEnglishComments
Ball Indentation Hardness 95.0 MPa13800 psiH358/30; ISO 2039-1
Tensile Strength 55.0 MPa7980 psiISO 527
Tensile Strength, Yield 55.0 MPa7980 psiISO 527
Elongation at Break 6.0 %6.0 %ISO 527
Elongation at Yield 3.0 %3.0 %ISO 527
Tensile Modulus 2.50 GPa363 ksiISO 527
Flexural Strength 78.0 MPa11300 psiISO 178
 75.0 MPa
@Strain 3.5 %
10900 psi
@Strain 3.5 %
ISO 178
Flexural Modulus 2.55 GPa370 ksiISO 178
Charpy Impact Unnotched  4.50 J/cm²
@Temperature -40.0 °C
21.4 ft-lb/in²
@Temperature -40.0 °F
ISO 179/1eU
 7.50 J/cm²
@Temperature -20.0 °C
35.7 ft-lb/in²
@Temperature -4.00 °F
ISO 179/1eU
 NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched  0.200 J/cm²
@Temperature -40.0 °C
0.952 ft-lb/in²
@Temperature -40.0 °F
ISO 179/1eA
 0.300 J/cm²
@Temperature -20.0 °C
1.43 ft-lb/in²
@Temperature -4.00 °F
ISO 179/1eA
 1.20 J/cm²
@Temperature 23.0 °C
5.71 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 90.0 °C194 °FISO 75-1/-2
Vicat Softening Point 102 °C216 °FB50; ISO 306
Flammability, UL94 HB
@Thickness 1.50 mm
HB
@Thickness 0.0591 in
Glow Wire Flammability Index  650 °C
@Thickness 1.00 mm
1200 °F
@Thickness 0.0394 in
passed; DIN EN 60695
 650 °C
@Thickness 2.00 mm
1200 °F
@Thickness 0.0787 in
passed; DIN EN 60695
 650 °C
@Thickness 3.00 mm
1200 °F
@Thickness 0.118 in
passed; DIN EN 60695
 
Processing PropertiesMetricEnglishComments
Melt Temperature 240 - 280 °C464 - 536 °FInjection molding
Mold Temperature 40.0 - 80.0 °C104 - 176 °FInjection molding
Drying Temperature  80.0 °C
@Time 7200 - 14400 sec
176 °F
@Time 2.00 - 4.00 hour
in a dry air (desiccant) dryer
 80.0 °C
@Time 10800 - 21600 sec
176 °F
@Time 3.00 - 6.00 hour
in an circulating dryer
 
Descriptive Properties
Base PolymerAcrylonitile/Sytrene/Acrylate/Coplymer

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Elix Polymers ELIX ABS E401 Acrylonitrile Butadiene Styrene (ABS), Extrusion, Impact Grade
A. Schulman Diamond Centrex® 825 Sheet Extrusion Grade
INEOS Styrolution Luran® S 757G ASA
Tabriz SH-0150 Extrusion Grade ABS
A. Schulman Diamond ASA 5946

PALBIS8629 / 242688

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.