MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

LyondellBasell Petrothene NA217000X01 Low Density Polyethylene (LDPE), Extrusion Grade  (discontinued **)
Categories: Polymer; Thermoplastic; Polyethylene (PE); Low Density (LDPE); Low Density Polyethylene (LDPE), Extrusion Grade

Material Notes: Petrothene NA217000X01 is a high speed, lightweight coating resin selected for use with paper, films and other base stocks. This resin can be extruded at line speeds of 1500 ft/min or higher. Products made from materials coated with NA217000X01 typically include flexible packaging, milk cartons, industrial papers and foil mounting, single-ply bags, pouch bags, cup stock, fiber drums, corrugated boxes and fiberboard containers. Applications: Bags & Pouches, Color Concentrates, Food Packaging Film, Lamination Film, Sealants.

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.923 g/cc0.0333 lb/in³ASTM D1505
Melt Flow 5.6 g/10 min
@Load 2.16 kg,
Temperature 190 °C
5.6 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 5353ASTM D2240
Tensile Strength at Break 12.4 MPa1800 psiType IV specimen; ASTM D638
Tensile Strength, Yield 13.0 MPa1890 psiType IV specimen; ASTM D638
Elongation at Break 550 %550 %Type IV specimen; ASTM D638
Elongation at Yield 13 %13 %Type IV specimen; ASTM D638
Flexural Modulus, 1% Secant 276 MPa40000 psiCrosshead speed of 0.5 inches/min; ASTM D790
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point 92.0 °C198 °FASTM D1525
 
Processing PropertiesMetricEnglishComments
Melt Temperature <= 329 °C<= 624 °F
 
Descriptive Properties
Processing MethodExtrusion Coating

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Bamberger Polymers Bapolene® 4062NA Polypropylene, Injection Grade
BP Amoco ACCPRO® 9644X Injection Grade Polypropylene
Ineos H00M-01 Polypropylene Homopolymer
LyondellBasell Alathon® H6018 High Density Polyethylene (Extrusion Grade)
LyondellBasell Alathon® M5370PX High Density Polyethylene, Extrusion Grade

PEQT8854 / 220488

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.