MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Elektro-Isola G-Etronax EP 311 EP368 Glass Fabric-Epoxy Laminate
Categories: Polymer; Thermoset; Epoxy; Epoxy/Glass SMC

Material Notes:

Information provided by Elektro-Isola

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.90 g/cc
@Temperature 23.0 °C
0.0686 lb/in³
@Temperature 73.4 °F
24h/23°C/50% RH; ISO 1183-A
Water Absorption 0.10 %0.10 %ISO 62-1
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 350 MPa
@Thickness >=1.50 mm
50800 psi
@Thickness >=0.0591 in
24h/23°C/50% RH; ISO 527
Flexural Strength  330 MPa
@Thickness >=1.50 mm,
Temperature 150 °C
47900 psi
@Thickness >=0.0591 in,
Temperature 302 °F
1 hour at temperature/50% RH, Normal to laminate plane; ISO 178
 480 MPa
@Thickness >=1.50 mm,
Temperature 23.0 °C
69600 psi
@Thickness >=0.0591 in,
Temperature 73.4 °F
24h/23°C/50% RH, Normal to laminate plane; ISO 178
Flexural Modulus 22.0 GPa
@Thickness >=1.50 mm
3190 ksi
@Thickness >=0.0591 in
24h/23°C/50% RH, Normal to laminate plane; ISO 178
Compressive Strength 600 MPa
@Thickness >=5.00 mm
87000 psi
@Thickness >=0.197 in
24h/23°C/50% RH, , Normal to laminate plane; ISO 604
Shear Strength 55.0 MPa
@Thickness >=5.00 mm
7980 psi
@Thickness >=0.197 in
Parallel, 24h/23°C/50% RH; IEC 60893-2
Izod Impact, Notched (ISO) 90.0 kJ/m²
@Thickness >=5.00 mm
42.8 ft-lb/in²
@Thickness >=0.197 in
Parallel, 24h/23°C/50% RH; ISO 180/2A
 
Electrical PropertiesMetricEnglishComments
Insulation Resistance 3.00e+8 ohm3.00e+8 ohmafter immersion in water for 24 hr at 23°C; IEC 60167
Dielectric Constant  5.0
@Thickness <=3.00 mm,
Frequency 50 Hz
5.0
@Thickness <=0.118 in,
Frequency 50 Hz
96h/105°C + 1h/23°C/20%RH; IEC 60250
 5.0
@Thickness <=3.00 mm,
Frequency 1e+6 Hz
5.0
@Thickness <=0.118 in,
Frequency 1e+6 Hz
96h/105°C + 1h/23°C/20%RH; IEC 60250
Dielectric Strength  2.76 kV/mm
@Thickness >=3.00 mm,
Temperature 90.0 °C
70.0 kV/in
@Thickness >=0.118 in,
Temperature 194 °F
after 1 hour in oil, Parallel to laminate plane; IEC 60243-1
 18.0 kV/mm
@Thickness 3.00 mm,
Temperature 90.0 °C
457 kV/in
@Thickness 0.118 in,
Temperature 194 °F
after 1 hour in oil, Normal to laminate plane; IEC 60243-1
Dissipation Factor  0.0050
@Thickness <=3.00 mm,
Frequency 50 Hz
0.0050
@Thickness <=0.118 in,
Frequency 50 Hz
96h/105°C + 1h/23°C/20%RH; IEC 60250
 0.0080
@Thickness <=3.00 mm,
Frequency 1e+6 Hz
0.0080
@Thickness <=0.118 in,
Frequency 1e+6 Hz
96h/105°C + 1h/23°C/20%RH; IEC 60250
Comparative Tracking Index 200 V
@Thickness >=3.00 mm
200 V
@Thickness >=0.118 in
24h/23°C/50% RH; IEC 60112
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 180 °C
@Thickness >=3.00 mm,
Time 7.20e+7 sec
356 °F
@Thickness >=0.118 in,
Time 20000 hour
IEC 60216
Flammability Test 5.0
@Thickness 3.00 mm
5.0
@Thickness 0.118 in
IEC 60695-11-10
Oxygen Index 44 %44 %
 
Descriptive Properties
ColorDark yellow

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Hexcel® F161 Epoxy Resin, 120 Glass Fabric
Hexcel® HexPly® F155 Epoxy Resin, 120 Glass Fabric
Applied Composites 8033 Polyester SMC
Applied Composites 8050 Polyester SMC
Elektro-Isola G-Etronax EP 10 Epoxy, Glass Fabric Reinforcement, Light Yellow, Sheets

PELEKT049m / 193448

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.