MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Armacell AP Armaflex® Coilflex Through 1" Duct Liner
Categories: Other Engineering Material

Material Notes: Elastomeric foam duct lining for energy efficiency, sustainability and the indoor environment.
  • Uniquely flexible and conformable for easier, labor-friendly fabrication:
    • The only elastomeric foam duct liner engineered for coil lines
    • Quick, gap-free, no-bulge bending on brake presses
    • Less cutting in hand assembly applications
  • Highest acoustic values of any elastomeric insulation: NRC 0.60 sound absorption, STC 25 noise blocking

Information provided by Armacell®

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Absorption Coefficient 0.520.52SAA
 0.60
@Thickness 1.00 mm
0.60
@Thickness 0.0394 in
NRC
 0.080
@Thickness 1.00 mm,
Frequency 125 Hz
0.080
@Thickness 0.0394 in,
Frequency 125 Hz
 0.22
@Thickness 1.00 mm,
Frequency 250 Hz
0.22
@Thickness 0.0394 in,
Frequency 250 Hz
 0.37
@Thickness 1.00 mm,
Frequency 1000 Hz
0.37
@Thickness 0.0394 in,
Frequency 1000 Hz
 0.50
@Thickness 1.00 mm,
Frequency 4000 Hz
0.50
@Thickness 0.0394 in,
Frequency 4000 Hz
 0.68
@Thickness 1.00 mm,
Frequency 2000 Hz
0.68
@Thickness 0.0394 in,
Frequency 2000 Hz
 1.03
@Thickness 1.00 mm,
Frequency 500 Hz
1.03
@Thickness 0.0394 in,
Frequency 500 Hz
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity  0.0360 W/m-K
@Temperature 24.0 °C
0.250 BTU-in/hr-ft²-°F
@Temperature 75.2 °F
ASTM C177 or C518
 0.0370 W/m-K
@Temperature 32.0 °C
0.257 BTU-in/hr-ft²-°F
@Temperature 89.6 °F
ASTM C177 or C518
Maximum Service Temperature, Air 82.0 °C180 °FASTM C534
Minimum Service Temperature, Air -183 °C-297 °FASTM C534
Flame Spread Index 2525ASTM E84
 
Descriptive Properties
Bacterial ResistancePassedASTM G22
Fungi ResistancePassedASTM G21/C1338
Mold GrowthPassedUL181
R-ValueR-4.21"
 R-61 1/2"
Smoke Developed Index50ASTM E84

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Rogers Corporation Bisco® A2 Sound Barrier Engineered Solid Silicone Mass Layer, Sound Barrier
Multibase Multi-Flex® TPE A 8699 BLK
Harris Acoustic Sensors E-1598 Gadolinium Substituted Garnet (8-series)
Armacell AP Armaflex® Coilflex Through 1 1/2" Duct Liner
Armacell AP Armaflex® 1 1/2" & 2" Duct Wrap

PARMD012 / 186623

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.