MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Wacker ELASTOSIL® LR 3003/90 A/B Liquid Silicone Rubber
Categories: Polymer; Thermoset; Silicone; Silicone Rubber; Liquid Silicone Rubber (LSR)

Material Notes: Liquid silicone rubbers of the ELASTOSIL® LR 3003 series are paste-like, easily-pigmentable two-component compounds with short curing times. Their vulcanizates are noted for their high transparency and excellent mechanical and electrical properties.

Properties: The products can be used within a temperature range of - 55 °C to + 210 °C. The addition of heat stabilizers at service temperatures of more than 180 °C is recommended.

Application: These grades are particularly suitable for the economical production of large series of injection-molded articles. Parts made from ELASTOSIL® LR 3003/90 A/B can be used for technical applications. These articles are also suitable for use in conjunction with foodstuffs. Postcured parts can be used for food contact applications and are suitable for use under the Recommendation "XV. Silicones" of the BfR and FDA § 177.2600 under observance of any given limitations on extractable and volatile substances.

Information provided by Wacker.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.14 g/cc1.14 g/ccISO 1183-1 A
Viscosity 800000 cP
@Shear Rate 0.890 1/s
800000 cP
@Shear Rate 0.890 1/s
DIN 53019
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 9090DIN 53505
Tensile Strength 8.00 MPa1160 psiDIN 53504 S 1
Elongation at Break 33 %33 %DIN 53504 S 1
Tear Strength 7.89 kN/m45.0 pliASTM D 624 B
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 210 °C410 °Fheat stabilizers recommended > 180°C
Minimum Service Temperature, Air -55.0 °C-67.0 °F
 
Optical PropertiesMetricEnglishComments
Transmission, Visible 90 %90 %Transparent, but not quantified
 
Processing PropertiesMetricEnglishComments
Cure Time 5.00 min
@Temperature 165 °C
0.0833 hour
@Temperature 329 °F
press cured, post cured 4 h/200 °C in ventilated air
 
Descriptive Properties
AppearanceTransparent

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Wacker ELASTOSIL® LR 3003/82 A/B Liquid Silicone Rubber
ExxonMobil Vistalon™ 805 EPDM Rubber
Wacker Elastosil® LR 3003/20 TR A/B Liquid Silicone Rubber
Wacker Elastosil® LR 3003/25 A/B Liquid Silicone Rubber
Wacker Elastosil® LR 3003/30 A/B Liquid Silicone Rubber

PWACK9926 / 197525

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.