MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Ice
Categories: Ceramic

Material Notes:

Key Words: Frozen Water (H2O)
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.897 g/cc0.0324 lb/in³
a Lattice Constant 4.5212 Å4.5212 Å
c Lattice Constant 7.3666 Å7.3666 Å
Formula Units/Cell (Z) 44
Molecular Weight 18.015 g/mol18.015 g/mol
Vapor Pressure 0.006105 bar
@Temperature 0.000 °C
4.579 torr
@Temperature 32.0 °F
 
Chemical PropertiesMetricEnglishComments
Critical Pressure 221.2 bar165900 torr
Critical Temperature 374.1 °C705.4 °F
 
Thermal PropertiesMetricEnglishComments
Heat of Fusion 333.5 J/g143.5 BTU/lb
Heat of Vaporization 2258 J/g971.3 BTU/lb
Specific Heat Capacity 2.10 J/g-°C
@Temperature -10.0 °C
0.502 BTU/lb-°F
@Temperature 14.0 °F
Melting Point 0.000 °C32.0 °F
Boiling Point 100 °C212 °F
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.311.31Average of several reported values
 
Descriptive Properties
Crystal StructureHexagonal

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Water, H2O
405 Stainless Steel
Aluminum 384.0-F Die Casting Alloy
Borosilicate Glass
Eastman Vanceva® Arctic Snow Colored Protective Interlayer for Architectural Glass

DWATI0 / 3093

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.