Hostacom T 30 T2 NERO is a 20% talc filled PP homopolymer, with medium melt flow rate and very good stiffness. The product is available in black color, pellet form. Applications: Automotive Parts, Instrument Panels, Under hoodInformation provided by LyondellBasell. |