MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

solder replacement adhesives

Superior Flux Superior No. 604B/3411 Boron-Modified Silver Brazing Paste Flux
Categories: Metal; Nonferrous Metal; Solder/Braze Alloy

Material Notes:
  • Boron-modified, high temperature silver brazing flux.
  • Brazes Copper, Brass, Nickel, carbon steel, stainless steel, and carbide.
  • Residues are water-soluble.
Superior No. 604B/3411 is a creamy, Boron-modified brazing paste flux that is active and protective to 925ºC/1,700ºF. It is formulated for brazing operations where a higher temperature or longer flux-life is necessary. It is recommended for use with copper and copper-based alloys, steel, stainless steel, nickel, carbides and heat-resistant alloys. Superior No. 604B/3411 is available in dispensable form suitable for spraying or other automatic application methods.

Applications: Superior No. 604B/3411 is a Boron-modified brazing flux used in a wide variety of joining applications for many different finished products including; carbide tools, stainless steel, large steel parts or processes requiring a long heating cycle.

Information provided by Superior Flux

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.60 g/cc1.60 g/cc
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 565 - 925 °C1050 - 1700 °FActive Range
 
Processing PropertiesMetricEnglishComments
Shelf Life 2.00 Month2.00 Month
 
Component Elements PropertiesMetricEnglishComments
H2O, Water 24 %24 %
 
Descriptive Properties
ColorDark Brown
FormCreamy Paste

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Zircar Refractory Composites RS-A1 Refractory Sheet
Sumitomo Bakelite Durez®-ter S105-30 Polyester Polyol
Solvay RHODASURF® T 50 Surfactant
Solvay MACKAM® C-37 Surfactant
Sharadaa Ceramics VELCRETE G 401 Gunning Castables

NSFLUX081 / 185765

Solder Replacement
RoHS Compliant Adhesives for Solder Replacement
Master Bond offers RoHS compliant, electrically conductive systems to replace lead soldering. These epoxy and silicone adhesives offer low volume resistivity, low outgassing and high temperature resistance.

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.