MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

Master Bond EP17HTDA-1 One component, high temperature epoxy system for bonding and sealing
Categories: Polymer; Thermoset; Epoxy; Epoxy, High Temperature

Material Notes: Key Features:
  • Ideal for die attach applications
  • Resists temperatures up to +600°F
  • Meets MIL-STD-883J Section 3.5.2 for thermal stability
  • Meets NASA low outgassing specifications
Master Bond EP17HTDA-1 is a one component, heat cured epoxy system primarily for die attach applications as well as more conventional bonding and sealing. It requires no mixing and cures readily at 300-350°F. Typical curing schedules are 2-3 hours at 300°F or 1-2 hours at 350°F. Curing in this manner will result in a glass transition temperature (Tg) of 195-205°C. EP17HTDA-1 has the ideal consistency and flow for die attach applications. This epoxy system features excellent physical properties, superb electrical insulation along with good thermal conductivity, even at elevated temperatures. This system is also distinctive in that it has a relatively low exotherm upon curing. EP17HTDA-1 is 100% reactive and contains no solvents or diluents. EP17HTDA-1 bonds well to similar and dissimilar substrates such as metal, ceramics, plastics and composites. It has a noteworthy resistance to many chemicals including acids, bases, salts, fuels, oils and many solvents. Significantly, it has minimal shrinkage upon curing. Its service temperature range is from -80°F to +600°F. Since it passes NASA low outgassing, it can be used in vacuum type situations and other applications where that requirement is needed. EP17HTDA-1 is used primarily as a die attach and adhesive/sealant in electronic and related applications, where high temperature resistance, good electrical insulation properties and thermal conductivity are desirable.

Product Advantages:

  • Single component system; no mixing prior to use
  • High temperature resistance
  • Very good electrical insulation properties, even at higher temperatures
  • Ideal viscosity flow profile for die attaching
  • Good thermal conductivity
  • Excellent die shear strength

Information provided by Masterbond.

Vendors: Master Bond is a leading manufacturer of adhesives, sealants, coatings and potting compounds. Master Bond’s vast product line consists of over 3,000 epoxy, polyurethane, silicone, cyanoacrylate and latex adhesives that vary in viscosity, cure speed, strength, chemical resistance, electrical properties, etc. Our custom adhesives offer design flexibility and provide excellent bonding performance. Visit www.masterbond.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.77 g/cc1.77 g/cc
Solids Content 100 %100 %
Viscosity 200000 - 2.50e+6 cP200000 - 2.50e+6 cPthixotropic
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 80 - 9080 - 90
Tensile Strength 62.1 - 68.9 MPa9000 - 10000 psi
Tensile Modulus 2.41 - 2.76 GPa350 - 400 ksi
Adhesive Bond Strength 16.5 - 17.9 MPa2400 - 2600 psilap shear, Al/Al
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+15 ohm-cm>= 1.00e+15 ohm-cm
Dielectric Constant 4.3
@Frequency 60 Hz
4.3
@Frequency 60 Hz
 
Thermal PropertiesMetricEnglishComments
CTE, linear 20.0 - 25.0 µm/m-°C11.1 - 13.9 µin/in-°F
Thermal Conductivity 1.4423 W/m-K10.010 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 316 °C600 °F
Minimum Service Temperature, Air -62.2 °C-80.0 °F
Glass Transition Temp, Tg 195 - 205 °C383 - 401 °F
 
Processing PropertiesMetricEnglishComments
Cure Time  60.0 - 120 min
@Temperature 177 °C
1.00 - 2.00 hour
@Temperature 350 °F
 120 - 180 min
@Temperature 149 °C
2.00 - 3.00 hour
@Temperature 300 °F
Shelf Life 3.00 - 6.00 Month
@Temperature 4.44 - 10.0 °C
3.00 - 6.00 Month
@Temperature 40.0 - 50.0 °F
in original syringes
 
Descriptive Properties
Coloramber
Die Shear Strength24-27 kg-f(2 x 2 mm [80 x 80 mil])
Thixotropic Index1.77
Typical die size4-400 mm2

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Epoxy, Molded, Mineral Filled
Master Bond EP17HTND-CCM One component, high temperature epoxy system for bonding and sealing
Lord Adhesives CoolTherm™ EP-2000 Thermally Conductive Epoxy Encapsulant
Epoxy Technology EPO-TEK® OE188 High Temperature Silica-Filled Epoxy
Cookson Group Plaskon® 435 Mineral Filled Epoxy Molding Compound

PMASTM706 / 233763

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.