MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Beijing Evergrow Resources PTFE, 15% Glass Fiber, 10% Polyimide, 5% Graphite Filled
Categories: Polymer; Thermoplastic; Fluoropolymer; Polytetrafluoroethylene (PTFE); Polytetrafluoroethylene (PTFE), Glass Filled, Molded

Material Notes: Filled PTFE article is manufactured by molding method with filled PTFE resin. Filled PTFE resin is manufactured by compounding PTFE granular resin with fillers of many different kinds. Amongst the many fillers suitable for compounding with PTFE, glass fiber, carbon fiber, Bronze and also lubricating materials like graphite, molybdenum disulphide, have been widely used in large scale production. Broadly speaking PTFE compounds have the following advantage over unfilled PTFE:

Improved compression strength
Improved thermal conductivity

Decreased thermal expansion

Improved abrasion resistance

Applications:
Packings

Information provided by Beijing Evergrow Resources.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break >= 10.0 MPa>= 1450 psi
Elongation at Break >= 120 %>= 120 %
Compressive Strength >= 16.7 MPa>= 2420 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Beijing Evergrow Resources PTFE, 20% Glass Fiber, 5% Graphite Filled
AGC Fluon® PA7115 15% Polyimide, PTFE Filled Compound
Ensinger Tecatron® XP-65 Compression Molded PPS Compound, 30% Fiberglass with 15% PTFE
Fluorseals PTFE 15% glass filled
AGC FC 174 PTFE, 15% Glass/ 5% Moly

PBEIJ037 / 90106

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.