MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Lubrizol STAT-RITE® S-1107 Static Dissipative TPU
Categories: Polymer; Thermoplastic; Elastomer, TPE; Polyurethane, TP

Material Notes: Description: Stat-Rite® S-1107 is a static dissipative TPU alloy. Stat-Rite S-1107 utilizes the patented Stat-Rite inherently dissipative polymer (IDP) alloy system to provide clean, permanent ESD protection. Stat-Rite® IDP alloys provide consistent static dissipation even when extruded, injection molded or thermoformed into components.

Features:

  • Permanent static dissipative
  • Humidity insensitive
  • Ultra-clean: low off-gassing, low ionic contamination
  • Colorable
  • Durable: Can be used for years and years

Applications:

  • ESD and Cleanroom Tubing
  • ESD and Cleanroom Hose
  • Cleanroom Curtains
  • Conveyor ESD Wear Strip, Rollers
  • ESD and Cleanroom Film

Available in Americas, Europe, Middle East, Africa, India and Asia

Information provided by Lubrizol.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.21 g/cc1.21 g/ccASTM D792
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 8383ASTM D2240
Tensile Strength 11.5 MPa1670 psiASTM D412
Tensile Stress at Strain  4.52 MPa
@Strain 50 %
656 psi
@Strain 50 %
ASTM D412
 5.21 MPa
@Strain 100 %
755 psi
@Strain 100 %
ASTM D412
 6.43 MPa
@Strain 200 %
933 psi
@Strain 200 %
ASTM D412
Elongation at Break 695 %695 %ASTM D412
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 2.30e+8 ohm-cm2.30e+8 ohm-cmASTM D257
Surface Resistance 4.80e+7 ohm4.80e+7 ohm12% RH; ESD S11.11
Surface Resistivity per Square 4.80e+8 ohm4.80e+8 ohm50%; ASTM D257
Static Decay 0.10 sec0.10 secCharged Plate Monitor, 50% RH (+1000 V to 100 V)
 <= 2.0 sec<= 2.0 sec12% RH (+5000 V to 50 V); FTMS-101C
 <= 2.0 sec<= 2.0 sec12% RH (-5000 V to -50 V); FTMS-101C
 
Processing PropertiesMetricEnglishComments
Drying Temperature 105 °C221 °Fdehumidifying hopper
Dry Time 2.00 - 3.00 hour2.00 - 3.00 hour
 
Descriptive Properties
ColorNatural

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Lubrizol STAT-RITE® S-1100 Static Dissipative TPU
Lubrizol STAT-RITE® E-1150 Ether-Type Static Dissipative Polymer
Lubrizol STAT-RITE® E-1140 Ester-Type Static Dissipative Polymer
Covestro Desmopan® 372 Thermoplastic Polyurethane
Sumitomo Bakelite North America RX® 660 Fiberglass Reinforced Phenolic Novolac

PNOVEON068b / 138282

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.