MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

LyondellBasell Higlass PF062-4 Polypropylene Homopolymer, 40% Glass Fiber  (discontinued **)
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes:
Key Features: high melt flow, high modulus, chemically coupled, glass fiber-reinforced polypropylene homopolymer, high rigidity, high strength, excellent processability

Applications: appliance parts, automotive components, electrical connectors

Description: Higlass PF062-4 high melt flow, chemically coupled, 40% glass fiber-reinforced polypropylene homopolymer has an excellent combination of strength, rigidity and processability.

Information provided by Montell Polyolefins.

LyondellBasell is the successor company to Montell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.22 g/cc0.0441 lb/in³ASTM D792
Linear Mold Shrinkage 0.0030 cm/cm0.0030 in/inTool, Montell
Melt Flow 17 g/10 min
@Load 2.16 kg,
Temperature 230 °C
17 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 100 MPa14500 psiASTM D638
Elongation at Break 2.0 %2.0 %ASTM D638
Flexural Modulus 6.90 GPa1000 ksiTangent at 0.05 in/min; ASTM D790A
Izod Impact, Notched 0.850 J/cm1.59 ft-lb/inASTM D256A
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 160 °C320 °FASTM D648

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LyondellBasell Higlass PF072-3 Polypropylene Homopolymer, 30% Glass Fiber
LyondellBasell Hostacom™ PF062-3 Polypropylene Homopolymer
LyondellBasell Higlass PF072-2 Polypropylene Homopolymer, 20% Glass Fiber
LyondellBasell Higlass PF062-2 Polypropylene Homopolymer, 20% Glass Fiber
LyondellBasell Astryn BC78A Polypropylene Copolymer, 23% Talc

PMO513 / 53660

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.