MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Garlock GYLON® 3594 PTFE Gasketing, Glass Fiber Filled
Categories: Polymer; Thermoplastic; Fluoropolymer; Polytetrafluoroethylene (PTFE); Polytetrafluoroethylene (PTFE), Glass Filled, Molded

Material Notes: PTFE with glass fiber filler

Information provided by Garlock Rubber Technologies

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Permeability 0.0150.015Gas Permeability, cc/min; DIN 3535 Part 4
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 13.8 MPa2000 psiacross grain; ASTM F152
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength 14.1 kV/mm
@Thickness 1.59 mm
357 kV/in
@Thickness 0.0625 in
Unconditioned; ASTM D149
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 260 °C
@Pressure 5.52 MPa
500 °F
@Pressure 800 psi
Continuous
Minimum Service Temperature, Air -268 °C-450 °F
 
Descriptive Properties
ColorGreen
Compressibility, %10-20ASTM F36
Creep Relaxation, %30ASTM F38
Sealability ASTM F37B, ml/hr0.5ASTM Fuel A

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Garlock GYLON® 3504 PTFE Gasketing, Glass Microsphere Filled

PGARL827 / 157502

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.