MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

3A Composites Core Materials BALTEK® SB.100 Structural End-Grain Balsa
Categories: Other Engineering Material; Composite Core Material; Polymer; Renewable/Recycled Polymer; Wood and Natural Products; Wood

Material Notes: BALTEK® SB is a core material produced from certified kiln-dried balsa wood in the ‘end-grain’ configuration. It has extremely high strength and stiffness to weight ratios, and achieves an excellent bond with all types of resins and adhesives. It is compatible with a variety of manufacturing processes and is resistant to temperature changes, or exposure to fire, or chemicals such as styrene. BALTEK® SB is an ideal core material for an extensive range of applications. All while being a renewable resource.

Characteristics:

  • Extremely high strength and stiffness to weight ratios
  • Excellent fire performance
  • Ecological product
  • Wide operating temperature range -212 °C to +163 ° C (-414 °F to +325 °F)
  • Excellent fatigue resistance
  • Good sound and thermal insulation
  • High impact strength
  • Good moisture resistance
Applications
  • Marine: Hulls, decks, bulkheads, superstructures, interiors, tooling + molds
  • Road and Rail: Floors, walls, roof panels, body panels, interiors, front-ends, side skirts
  • Wind Energy: Rotor blades, spinners, nacelle covers, generator housings
  • Aircraft: Floor panels, galley carts, interior partitions, cargo pallets, containers, general aviation (sport aircraft) parts
  • Defense: Naval vessels, containers, cargo pallets, shelters
  • Industrial: Tooling, tanks, ductwork, impact limiter, concrete forms, fascia panels, skis, snowboards, wakeboards
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.153 g/cc0.00553 lb/in³apparent nominal; ASTM C271
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 13.2 MPa1910 psiperpendicular to plane; ASTM C297
Tensile Modulus 3.57 GPa518 ksiperpendicular to plane; ASTM C297
Compressive Strength 12.9 MPa1870 psiperpendicular to plane; ASTM C365
Compressive Modulus 4.005 GPa580.9 ksiperpendicular to plane; ASTM C365
Shear Modulus 0.160 GPa23.2 ksiASTM C273
Shear Strength 3.00 MPa435 psiASTM C273
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 0.0660 W/m-K0.458 BTU-in/hr-ft²-°FASTM C177

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
3A Composites Core Materials BALTEK® SB.150 Structural End-Grain Balsa
3A Composites Core Materials BALTEK® SB.50 Structural End-Grain Balsa
Carbon-Core Carbon Balsa Wood
CoreLite BALSASUD® Core SG Standard Grade Balsa Core Material
3A Composites Core Materials AIREX® C51.60 Industrial Processing Foam

PZ3AC002 / 108491

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.