MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Plastcom SLOVAMID 6 GF 10 FRC 2 PA6, 10% glass fibre, flame retardant
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 10% Glass Fiber Filled; Nylon 6, Glass Fiber Filled, Flame Retardant

Material Notes: Features

PA 6 for injection moulding, chemically strengthened with 10 % glass fibre. Application: impacted mouldings and mouldings with high strength applied in automotive, electrical, engineering and consumer-goods industry, eg.: grips for electro tools, hobby tools, gears, cases of the electrotools, cooling skrews of blowers, electromotors, carrying parts in the automotive industry. With the increasing content of GF also the toughness, bending and tensile strength increase as well as the heat application increases up to 250°C and the shrinkage decreases. Delivered in natural mode and in the full RAL colour scale.

Packaging, transport, stocking

The product is packed in hermetically closed thick-walled 25 kg PE bags, on a 1.000 kg palette coated in a stretch foil, in big bags with a thick PE foil fixed on a 1.000 kg palette, in paper octabins with a thick PE foil fixed on a 1.000 kg palette or in other packaging according to customer requirements. The transport is provided in closed-up vehicles where the material is protected against movement and mechanical damage. The product requires stocking in closed-up, dry places protected against sun and thermal radiation.

Information Provided by Plastcom spol. s r.o.

Key Words: PA6
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.23 g/cc0.0444 lb/in³
Viscosity Measurement 0.67 - 1.580.67 - 1.58
Linear Mold Shrinkage 0.0067 cm/cm0.0067 in/in
Linear Mold Shrinkage, Transverse 0.0158 cm/cm0.0158 in/in
Melt Flow 3.0 g/10 min
@Load 0.325 kg,
Temperature 270 °C
3.0 g/10 min
@Load 0.716 lb,
Temperature 518 °F
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 90.0 MPa13100 psi
Elongation at Break 4.0 %4.0 %
Tensile Modulus 5.80 GPa841 ksi
Flexural Strength 160 MPa23200 psi
Flexural Modulus 4.80 GPa696 ksi
Charpy Impact Unnotched  2.00 J/cm²
@Temperature -20.0 °C
9.52 ft-lb/in²
@Temperature -4.00 °F
 2.50 J/cm²
@Temperature 23.0 °C
11.9 ft-lb/in²
@Temperature 73.4 °F
Charpy Impact, Notched  0.200 J/cm²
@Temperature -20.0 °C
0.952 ft-lb/in²
@Temperature -4.00 °F
 0.300 J/cm²
@Temperature 23.0 °C
1.43 ft-lb/in²
@Temperature 73.4 °F
 
Thermal PropertiesMetricEnglishComments
Melting Point 220 °C428 °F
Deflection Temperature at 1.8 MPa (264 psi) 200 °C392 °F
Vicat Softening Point 200 °C392 °FB
Flammability, UL94 V-2V-2
Glow Wire Test 850 °C1560 °F
 
Processing PropertiesMetricEnglishComments
Melt Temperature 250 - 270 °C482 - 518 °F
Mold Temperature 70.0 - 80.0 °C158 - 176 °F
Drying Temperature 80.0 °C176 °F
Dry Time 4 hour4 hour
Moisture Content 0.15 %0.15 %
Injection Pressure 70.0 - 120 MPa10200 - 17400 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Polyplastic Armamid® PA GF25-1FR Nylon 6, 25% Glass Fiber
Plastcom SLOVAMID 6 GF 15 Polyamide 6, 15% Glass Fiber
Plastcom SLOVAMID 6 GF 15 FRA 5 Polyamide 6, 15% Glass Fiber, Halogen Flame Retardant
Plastcom SLOVAMID 6 GF 10 FRG 5 Polyamide 6, 10% Glass Fiber, Flame Retardant
Envalior Novamid® 1010GN2-20 NAT/BK37 PA6-GF20 FR(17)

PPLACO320 / 120944

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.