Flexirene CL 10 U is a butene copolymer linear low density polyethylene (C4-LLDPE), with antioxidants, suitable for cast extrusion of thin film with high optical properties. Main Applications: Flexirene CL 10 U is recommended for the production of stretch film to be used in both manual and automatic wrapping machines. In a multilayer film, Flexirene CL 10 U enhances the optical properties of the global formulation; moreover, for its high processability, the resin is recommended whenever high productivity has to be reached. Information provided by Polimeri Europa. Versalis is the Eni subsidiary containing the plastics and rubber businesses. |