MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Chemours Viton® GBLT-600S with Wollastonite Fluoroelastomer Compound
Categories: Polymer; Thermoset; Fluoropolymer, TS; Thermoset Fluoroelastomer; Rubber or Thermoset Elastomer (TSE)

Material Notes:
  • GBLT-600S is an alternative to GLT and GFLT for fuel seals and fuel injector O-rings
  • Good fuel, methanol, and fluids resistance, improved vs. GLT
  • Low temperature Tg, TR-10, and sealing improved vs. Viton® GFLT
  • Heat resistance comparable to Viton® GLT-600S and GFLT-600S Good mold release / mold fouling properties
  • Good physical properties with high elongation, both original and aged
  • Good water and steam resistance / low volume swell in water
  • Excellent compression set resistance with either low or no postcure F169

Chemours was formed from former DuPont performance chemicals businesses, including the Viton product line, in 2015.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 6666No Postcure; ASTM D1414
 69692 hours Postcure; ASTM D1414
Tensile Strength at Break 7.80 MPa1130 psiNo Postcure
 8.70 MPa1260 psi2 hours Postcure
Tensile Stress at Strain  1.00 MPa
@Strain 10 %
145 psi
@Strain 10 %
No Postcure; ASTM D412
 1.00 MPa
@Strain 10 %
145 psi
@Strain 10 %
Postcured; ASTM D412
Elongation at Break 260 %260 %2 hours Postcure; ASTM D412
 297 %297 %No Postcure; ASTM D412
100% Modulus  4.10 MPa
@Strain 100 %
595 psi
@Strain 100 %
No Postcure; ASTM D412
 5.50 MPa
@Strain 100 %
798 psi
@Strain 100 %
Postcured; ASTM D412
Compression Set  11 %
@Temperature 200 °C,
Time 79200 sec
11 %
@Temperature 392 °F,
Time 22.0 hour
Plied Discs, postcured; ASTM D395B
 14 %
@Temperature 200 °C,
Time 79200 sec
14 %
@Temperature 392 °F,
Time 22.0 hour
O-Rings, postcured; ASTM D395B
 16 %
@Temperature 200 °C,
Time 252000 sec
16 %
@Temperature 392 °F,
Time 70.0 hour
Plied Discs, postcured; ASTM D395B
 21 %
@Temperature 200 °C,
Time 79200 sec
21 %
@Temperature 392 °F,
Time 22.0 hour
O-Rings, no postcure; ASTM D395B
 23 %
@Temperature 200 °C,
Time 252000 sec
23 %
@Temperature 392 °F,
Time 70.0 hour
O-Rings, postcured; ASTM D395B
 29 %
@Temperature 200 °C,
Time 252000 sec
29 %
@Temperature 392 °F,
Time 70.0 hour
O-Rings no postcure; ASTM D395B
 
Thermal PropertiesMetricEnglishComments
Minimum Service Temperature, Air -26.1 °C-15.0 °FRetraction Temperature, Tr10; ASTM D1329
Glass Transition Temp, Tg -27.4 °C-17.3 °F
 
Processing PropertiesMetricEnglishComments
Processing Temperature  177 °C
@Time 421 sec
351 °F
@Time 0.117 hour
Cure
 232 °C
@Time 7200 sec
450 °F
@Time 2.00 hour
Postcure
 
Component Elements PropertiesMetricEnglishComments
Fluorine, F 66 %66 %Uncompounded Viton
 
Descriptive Properties
Compound NumberA14-04
Formulation as Tested0.5Armeen® 18D
 1.5Varox® DBPH-50
 100GBLT-600S
 3Zinc Oxide
 3Diak 7 (TAIC)
 40Wollastocoat® 10222

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Chemours Viton® GBLT-600S Fluoroelastomer Compound
Chemours Viton® GBLT-600S with 30-MT Black Fluoroelastomer Compound
Chemours Viton® GBLT-600S with 60-MT Black Fluoroelastomer Compound
Chemours Viton® GLT-200S Fluoroelastomer Compound
Chemours Viton® GBL-200S Fluoroelastomer Compound

PDVC9805 / 170446

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.