MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Electrolytic Tough Pitch (ETP) Copper, UNS C11000, OSO50 Temper wire
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: Good to excellent corrosion resistance. Excellent hot and cold workability; good forgeability. Fabricated by coining, coppersmithing, drawing and upsetting, hot forging and pressing, spinning, swaging, stamping.

Applications: downspouts, gutters, roofing, gaskets, auto radiators, busbars, nails, printing rolls, rivets, and radio parts.

Test specimens: wire - 2mm diameter.

Key Words: ASTM-B-152, QQ-C-576, CDA 110 ETP, C101, ISO Cu-ETP
Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 8.89 g/cc0.321 lb/in³
 7.93 g/cc
@Temperature 1083 °C
0.286 lb/in³
@Temperature 1981 °F
Liquid
 8.32 g/cc
@Temperature 1083 °C
0.301 lb/in³
@Temperature 1981 °F
Solid
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 240 MPa34800 psi
 235 MPa
@Temperature -40.0 °C
34100 psi
@Temperature -40.0 °F
 260 MPa
@Temperature -75.0 °C
37700 psi
@Temperature -103 °F
 285 MPa
@Temperature -120 °C
41300 psi
@Temperature -184 °F
 320 MPa
@Temperature 12.0 °C
46400 psi
@Temperature 53.6 °F
 325 MPa
@Temperature -12.0 °C
47100 psi
@Temperature 10.4 °F
 400 MPa
@Temperature -175 °C
58000 psi
@Temperature -283 °F
Tensile Strength, Yield  65.0 MPa
@Strain 0.1 %,
Temperature 0.000 °C
9430 psi
@Strain 0.1 %,
Temperature 32.0 °F
 70.0 MPa
@Strain 0.1 %,
Temperature -50.0 °C
10200 psi
@Strain 0.1 %,
Temperature -58.0 °F
 75.0 MPa
@Strain 0.1 %,
Temperature -100 °C
10900 psi
@Strain 0.1 %,
Temperature -148 °F
 80.0 MPa
@Strain 0.1 %,
Temperature -150 °C
11600 psi
@Strain 0.1 %,
Temperature -238 °F
Elongation at Break 35 %35 %in 250 mm
 40 %
@Temperature -12.0 °C
40 %
@Temperature 10.4 °F
 45 %
@Temperature -120 °C
45 %
@Temperature -184 °F
 47 %
@Temperature 12.0 °C
47 %
@Temperature 53.6 °F
 48 %
@Temperature -75.0 °C
48 %
@Temperature -103 °F
 48 %
@Temperature -40.0 °C
48 %
@Temperature -40.0 °F
 57 %
@Temperature -175 °C
57 %
@Temperature -283 °F
Reduction of Area  70 %
@Temperature -120 °C
70 %
@Temperature -184 °F
 74 %
@Temperature -75.0 °C
74 %
@Temperature -103 °F
 76 %
@Temperature 12.0 °C
76 %
@Temperature 53.6 °F
 77 %
@Temperature -175 °C
77 %
@Temperature -283 °F
 77 %
@Temperature -40.0 °C
77 %
@Temperature -40.0 °F
 78 %
@Temperature -12.0 °C
78 %
@Temperature 10.4 °F
Modulus of Elasticity 115 GPa16700 ksiO60 temper
Poissons Ratio 0.330.33
Machinability 20 %20 %UNS C36000 (free-cutting brass) = 100%
Forgeability 65 %65 %UNS C37700 (forging brass) = 100%
Shear Modulus 44.0 GPa6380 ksiO60 temper
Shear Strength 165 MPa23900 psi
Coefficient of Friction, Dynamic 0.290.29Sliding, with cast iron, no lubrication
 0.360.36Sliding, with carbon steel, no lubrication
 0.530.53Sliding, with glass, no lubrication
Coefficient of Friction, Static 0.530.53With carbon steel, no lubrication
 0.680.68With carbon steel, no lubrication
 1.051.05With cast iron, no lubrication
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000170 ohm-cm0.00000170 ohm-cm101% IACS
 
Thermal PropertiesMetricEnglishComments
Heat of Fusion 205 J/g88.2 BTU/lb
CTE, linear  17.0 µm/m-°C
@Temperature 20.0 - 100 °C
9.44 µin/in-°F
@Temperature 68.0 - 212 °F
 17.3 µm/m-°C
@Temperature 20.0 - 200 °C
9.61 µin/in-°F
@Temperature 68.0 - 392 °F
 17.7 µm/m-°C
@Temperature 20.0 - 300 °C
9.83 µin/in-°F
@Temperature 68.0 - 572 °F
Specific Heat Capacity 0.385 J/g-°C0.0920 BTU/lb-°F
Thermal Conductivity  300 W/m-K
@Temperature -268.8 °C
2080 BTU-in/hr-ft²-°F
@Temperature -451.8 °F
 300 W/m-K
@Temperature 700 °C
2080 BTU-in/hr-ft²-°F
@Temperature 1290 °F
 370 W/m-K
@Temperature 300 °C
2570 BTU-in/hr-ft²-°F
@Temperature 572 °F
 380 W/m-K
@Temperature 100 °C
2640 BTU-in/hr-ft²-°F
@Temperature 212 °F
 388 W/m-K
@Temperature 20.0 °C
2690 BTU-in/hr-ft²-°F
@Temperature 68.0 °F
 390 W/m-K
@Temperature 0.000 °C
2710 BTU-in/hr-ft²-°F
@Temperature 32.0 °F
 400 W/m-K
@Temperature -79.0 °C
2780 BTU-in/hr-ft²-°F
@Temperature -110 °F
 550 W/m-K
@Temperature -196 °C
3820 BTU-in/hr-ft²-°F
@Temperature -321 °F
 1300 W/m-K
@Temperature -253 °C
9020 BTU-in/hr-ft²-°F
@Temperature -423 °F
Melting Point 1065 - 1083 °C1949 - 1981 °F
Solidus 1065 °C1949 °FEutectic
Liquidus 1083 °C1981 °F
Softening Point 360 °C680 °F
Annealing Point >= 371 °C>= 700 °F
 
Processing PropertiesMetricEnglishComments
Annealing Temperature 475 - 750 °C887 - 1380 °F
Hot-Working Temperature 750 - 875 °C1380 - 1610 °F
 
Component Elements PropertiesMetricEnglishComments
Copper, Cu >= 99.90 %>= 99.90 %includes Ag
Oxygen, O 0.040 %0.040 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Electrolytic Tough Pitch (ETP) Copper, UNS C11000, H04 Temper wire
Electrolytic Tough Pitch (ETP) Copper, UNS C11000, H08 Temper wire
Electrolytic Tough Pitch (ETP) Copper, UNS C11000, OSO50 Temper flat products, rod, tube, shapes
Electrolytic Tough Pitch (ETP) Copper, UNS C11000, OSO25 Temper flat products, tube
Electrolytic Tough Pitch (ETP) Copper, UNS C11000, H00 Temper flat products

MC11000c2 / 10498

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.