MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Mitsubishi Iupiace® EHM103R m-Polyphenylene Ether (m-PPE)
Categories: Polymer; Thermoplastic; Polyphenylene Ether/PPO

Material Notes: Anti-static grade. Iupiace is a polymer alloy made by modifying PPE with high impact polystyrene (HIPS), nylon-6 or nylon-66. Usability in a wide range of temperatures (-40 to 160). Higher rigidity, impact strength and fatigue resistance. Excellent insulation properties, low dielectric constant and low dielectric dissipation factor. Excellent dimensional stability with low water absorption. Flame retardance and excellent self-extinguishing properties. Low density. Low shrinkage rate, ensuring quality precision parts. Good mold release, easy flow properties and a wide range of stock temperatures.

Information provided by Mitsubishi Engineering Plastics Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.16 g/cc0.0419 lb/in³ISO 1183
Linear Mold Shrinkage, Flow 0.0085 - 0.0105 cm/cm
@Thickness 3.20 mm
0.0085 - 0.0105 in/in
@Thickness 0.126 in
Linear Mold Shrinkage, Transverse 0.0085 - 0.0105 cm/cm
@Thickness 3.20 mm
0.0085 - 0.0105 in/in
@Thickness 0.126 in
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 62.0 MPa8990 psiISO 527-1,2
Elongation at Break 8.0 %8.0 %ISO 527-1,2
Tensile Modulus 2.60 GPa377 ksiISO 527-1,2
Flexural Strength 105 MPa15200 psiISO 178
Flexural Modulus 2.70 GPa392 ksiISO 178
Charpy Impact Unnotched <= 4.00 J/cm²<= 19.0 ft-lb/in²ISO 179-1,2
 
Electrical PropertiesMetricEnglishComments
Surface Resistance 2000 ohm2000 ohmIEC 60093
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 160 °C320 °F
Deflection Temperature at 0.46 MPa (66 psi) 160 °C320 °FISO 75-1,2
Deflection Temperature at 1.8 MPa (264 psi) 150 °C302 °FISO 75-1,2
Minimum Service Temperature, Air -40.0 °C-40.0 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BASF Luranyl® KR 2403 G2 Polyphenylene Ether + Styrene-Butadiene Blend, 10% Glass Fiber Reinforced
Mitsubishi Iupiace® AP6GM2 m-Polyphenylene Ether (m-PPE)
Mitsubishi Iupiace® AP6GM4 m-Polyphenylene Ether (m-PPE)
BASF Luranyl® KR 2401 Polyphenylene Ether + Styrene-Butadiene Blend, Impact Grade
BASF Luranyl® KR 2420 Polyphenylene Ether + Styrene-Butadiene Blend

PMITSU9102 / 191775

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.