MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Formosa Plastics Formolon® 616K PVC
Categories: Polymer; Thermoplastic; Vinyl (PVC); PVC, Molded

Material Notes: PVC Homopolymer General Purpose Grade Resin

F616K is a medium-low molecular weight PVC homopolymer of particular interest in rigid applications and has established a deserved reputation for low gels and exceptional early color heat stability. These properties, along with outstanding lot to lot uniformity have made F616K an industry wide standard for rigid formulations.

Applications: Rigid Calendering, Rigid Foam, Profile and Bottles.

ASTM Classification: GP3-16000, ASTM D1755

Information provided by Formosa Plastics Corporation, USA

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.550 g/cc0.0199 lb/in³ASTM D1895
Volatiles 0.20 %0.20 %ASTM D6980
Particle Mesh Size 40 Mesh40 Mesh99.9% thru; Malvern
 200 Mesh200 Mesh4% thru; Malvern
Viscosity 0.79 cP0.79 cPInherent; ASTM D5225
Relative Viscosity 1.96 cP1.96 cP
 
Descriptive Properties
Composition<1.0 ppmResidual VCM, GC Head Space Method
 20Contamination Count, OCS per 100g
K-Value61Fikentscher's Constant

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Formosa Plastics Formolon® 40 PVC
Formosa Plastics Formolon® 10 PVC
Fainplast Compounds PK 71/FR Flexible PVC, Lead Free
Fainplast Compounds PK 7015/UV Flexible PVC, Lead Free
Fainplast Compounds PK 100 Flexible PVC, Lead Free

PFPCPQ082 / 150314

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.