MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Syensqo (Solvay Specialty Polymers) Cogegum® AFR/720 Polyolefin  (discontinued **)
Categories: Polymer; Thermoplastic; Polyolefin

Material Notes: Cogegum® HFFR -Halogen Free Fire Retardant compound Polyolefin based thermoplastic compound containing a fire retardant system that contributes to give the cable self-extinguish properties without halogenidric acids evolution; furthermore, toxic and corrosive gases emission and smoke generation are particularly reduced. These characteristics make this compound suitable in all applications where the fire behavior of cable materials is one of the main concerns to be considered in establishing a high safety level in public places. This material complies with RoHS requirements. standard complying - EN 50363-0 M1, M9; EN 50363-7 TI6, TI7; IEC 60502-1 ST8; Cenelec HD 624.7 S1; Cenelec HD 624.6 S1; VDE 0207 HM2, HM5, HJ2; IEC 60092 SHF1; UNE 211002 TIZ1; UNE 21123-4

Additional Information: Tests reported are performed on pressed or extruded specimens Coloring - EVA or PE based masterbatches added at 1.2-1.5% by weight; in order to avoid scotching problems during processing, predrying of colour masterbatch is suggested if moisture absorption occurred during storage (4-6 hours at 50-60°C). Storage - The product must be stored under the following conditions: -- closed and undamaged bags -- ambient temperature not exceeding 35°C -- avoid direct exposure to sunlight and weathering - Product alterations could occur due to extended period of storage - Shelf life: 12 months - Solvay Specialty Polymers accepts no liability of any kind in case the above mentioned conditions are not fulfilled. Packaging - 25 kg moisture-resistant bags on 1375 kg pallet - 1000 kg carton box

Extrusion Notes: Extrusion equipment - standard extruders for thermoplastics equipped with low compression screw (1:1.2-1.4 compression ratio and 20-25 L/D ratio are suggested), and an adequate barrel thermoregulation - don't use screw thermoregulation - filter net: not necessary; in case, use 40-80 mesh/cm² max. Anyway the use of the breaker plate is advisable, in particular using low compression screws

Information provided by Solvay Specialty Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.48 g/cc1.48 g/ccASTM D792
ESCR 10% Igepal® 1000 hour
@Thickness 3.00 mm,
Temperature 50.0 °C
1000 hour
@Thickness 0.118 in,
Temperature 122 °F
Condition A, Compression Molded; ASTM D1693
Melt Flow 3.9 g/10 min
@Load 21.6 kg,
Temperature 150 °C
3.9 g/10 min
@Load 47.6 lb,
Temperature 302 °F
Internal Method
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 4747ISO 868
Tensile Strength at Break 15.2 MPa2200 psiIEC 60811
Elongation at Break 190 %190 %IEC 60811
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity  5.50e+12 ohm-cm
@Temperature 70.0 °C
5.50e+12 ohm-cm
@Temperature 158 °F
IEC 60502
 4.10e+14 ohm-cm
@Temperature 20.0 °C
4.10e+14 ohm-cm
@Temperature 68.0 °F
IEC 60502
Insulation Resistivity  20.0 Megaohm/1000 m
@Temperature 70.0 °C
65.6 Megaohm/1000 ft
@Temperature 158 °F
IEC 60502
 1500 Megaohm/1000 m
@Temperature 20.0 °C
4920 Megaohm/1000 ft
@Temperature 68.0 °F
IEC 60502
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 280 °C536 °FTemperature Index (Burning); NES 715
Oxygen Index 39 %39 %ASTM D2863
 
Processing PropertiesMetricEnglishComments
Processing Temperature 150 - 170 °C302 - 338 °FCollar Temperature
Zone 1 130 - 150 °C266 - 302 °F
Zone 2 130 - 160 °C266 - 320 °F
Zone 3 140 - 160 °C284 - 320 °F
Zone 4 140 - 160 °C284 - 320 °F
Die Temperature 150 - 180 °C302 - 356 °F
Head Temperature 150 - 170 °C302 - 338 °F
 
Descriptive Properties
AvailabilityAsia Pacific
 Europe
 North America
Bending TestPass-25°C; IEC 60811
Calorific Potential16.2 MJ/kgISO 1716; Upper (gross)
Cold ImpactPassIEC 60811; -25°C
Corrosive Gas in Smoke< 10.0 µS/mmConductivity IEC 60754-2
 pH > 4.30
FeaturesFlame Retardant
 Halogen Free
 Low Smoke Emission
 Low Toxicity
 Self Extinguishing
GenericPolyolefin, Unspecified
Halogenidric Acid Emissions< 0.10%
Heat ShockPassIEC 60811; 150°C
Hot Pressure Test< 50%90°C; max penetration, K=0.6; IEC 60811
Hydrocarbons Immersion Test, 25°C, 4 hr-12CEI 20-34/0-1; % Change in Tensile Strength
 -5CEI 20-34/0-1; % Change in Tensile Elongation
Mechanical Properties After Aging in Air Oven, 100°C, 168 hr-10IEC 60811, %Change in Tensile Elongation
 4IEC 60811, %Change in Tensile Strength
Mechanical Properties After Aging in Air Oven, 80°C, 168 hr-12IEC 60811, %Change in Tensile Elongation
 -5IEC 60811, %Change in Tensile Strength
RoHS ComplianceRoHS Compliant
SAE 20 Oil Immersion Test, 70°C, 4 hr-24% Change in Tensile Strength
 4% Change in Tensile Elongation
UsesCable Jacketing
 Low Voltage Insulation
 Wire & Cable Applications
Water Absorption (mg/cm²)3.5100°C; 24 hr; IEC 60811

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ExxonMobil Escorene™ Ultra LD 726.07 Ethylene Vinyl Acetate Copolymer (EVA), Extrusion/Coating Grade
ExxonMobil Escorene™ Ultra UL 7765 Ethylene Vinyl Acetate Copolymer (EVA), Adhesive/Sealant Grade
ExxonMobil Escorene® LD-409 EVA for Low Voltage Insulation
ExxonMobil Escorene® LD-401 EVA for Electrical Insulation
DuPont Elvax® 40L-08 Ethylene-Vinyl Acetate Copolymer Resin

PSOL8Y7618 / 135681

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.