MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Precision Polymer Engineering N70N Nitrile Rubber
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Nitrile Butadiene Rubber (NBR) 66-75 °IRHD. Copolymer of acrylonitrile and butadiene. To meet Aerospace Material Specification DTD5595A Grade 70.

Applications: Synthetic rubber resistant to petroleum-based fuels and diester-based lubricants. Unsuitable for use in contact with phosphate ester hydraulic fluids.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 7070°IRHD; ASTM D1415
 70 - 7870 - 78°IRHD, -0/+8 change after 168 hours @ 100°C; ASTM D1415
Tensile Strength, Yield 9.45 MPa1370 psi-10% change after 168 hours @ 100°C; ASTM D412
 10.5 MPa1520 psiASTM D412
Elongation at Break 161 %161 %-30% change after 168 hours @ 100°C; ASTM D412
 230 %230 %ASTM D412
Compression Set 13.5 %
@Temperature 100 °C,
Time 86400 sec
13.5 %
@Temperature 212 °F,
Time 24.0 hour
ASTM D395
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 150 °C302 °F
Minimum Service Temperature, Air -40.0 °C-40.0 °F
 -25.0 °C-13.0 °FTemperature at which stiffness does not exceed 70 Mpa
Flash Point >= 300 °C>= 572 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Precision Polymer Engineering N70C Nitrile Rubber
Precision Polymer Engineering N60K Nitrile Rubber
Precision Polymer Engineering N70F Nitrile Rubber
Precision Polymer Engineering N70H Nitrile Rubber
Precision Polymer Engineering N70J Nitrile Rubber

PPRECI192 / 57916

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.