MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Carbon Monoxide, CO
Categories: Fluid

Material Notes: CAS Number: 630-08-0

Physical Form: Colorless Gas

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.001145 g/cc0.00004137 lb/in³Gas
Molecular Weight 28.01 g/mol28.01 g/mol
 
Chemical PropertiesMetricEnglishComments
Critical Pressure 34.9900 bar26244.7 torr
Critical Temperature -140.09 °C-220.16 °F
Critical Molar Volume 93.0 cm³/mol5.68 in³/mol
 
Thermal PropertiesMetricEnglishComments
Heat of Fusion 29.74 J/g12.79 BTU/lb
Heat of Vaporization 215.6 J/g92.77 BTU/lbAt Boiling Point
Specific Heat Capacity 1.039 J/g-°C0.2483 BTU/lb-°FGas
Thermal Conductivity  0.0250 W/m-K
@Pressure 0.000 MPa,
Temperature 26.9 °C
0.174 BTU-in/hr-ft²-°F
@Pressure 0.000 psi,
Temperature 80.3 °F
gas; low pressure limiting value
 0.0323 W/m-K
@Pressure 0.000 MPa,
Temperature 127 °C
0.224 BTU-in/hr-ft²-°F
@Pressure 0.000 psi,
Temperature 260 °F
gas; low pressure limiting value
 0.0392 W/m-K
@Pressure 0.000 MPa,
Temperature 227 °C
0.272 BTU-in/hr-ft²-°F
@Pressure 0.000 psi,
Temperature 440 °F
gas; low pressure limiting value
 0.0457 W/m-K
@Pressure 0.000 MPa,
Temperature 327 °C
0.317 BTU-in/hr-ft²-°F
@Pressure 0.000 psi,
Temperature 620 °F
gas; low pressure limiting value
Melting Point -205 °C-337 °F
Boiling Point -191.5 °C-312.7 °F
Heat of Formation -110.5 kJ/mol-110.5 kJ/molGas
 
Descriptive Properties
SolubilitySlightly Soluble in H2O; Soluble in Chloroform and EtOH

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Nitrous Oxide, N2O, Nitrogen Dioxide

EINOR2356 / 4485

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.