MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Copper, UNS C19200, H04 Temper strip
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: Good to excellent corrosion resistance. Excellent hot and cold workability. Applications include automotive hydraulic brake lines, flexible hose, electrical terminals, fuse clips, gaskets, gift hollow ware, applications requiring resistance to softening and stress corrosion, air conditioning and heat exchanger tubing.

Test specimen: strip - 1mm diameter.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.87 g/cc0.320 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell B 7272
Tensile Strength, Ultimate 450 MPa65300 psi
Tensile Strength, Yield 415 MPa
@Strain 0.2 %
60200 psi
@Strain 0.2 %
Elongation at Break 7.0 %7.0 %In 50 mm
Modulus of Elasticity 115 GPa16700 ksi
Poissons Ratio 0.3070.307
Machinability 20 %20 %
Forgeability 65 %65 %
Shear Modulus 44.0 GPa6380 ksi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000288 ohm-cm
@Temperature 20.0 °C
0.00000288 ohm-cm
@Temperature 68.0 °F
 
Thermal PropertiesMetricEnglishComments
CTE, linear 16.2 µm/m-°C
@Temperature 20.0 - 100 °C
9.00 µin/in-°F
@Temperature 68.0 - 212 °F
Specific Heat Capacity 0.380 J/g-°C0.0908 BTU/lb-°F
Thermal Conductivity 251 W/m-K1740 BTU-in/hr-ft²-°F
Melting Point 1078 - 1084 °C1972 - 1983 °F
Solidus 1078 °C1972 °F
Liquidus 1084 °C1983 °F
Annealing Point 704 - 816 °C1300 - 1500 °F
 
Processing PropertiesMetricEnglishComments
Annealing Temperature 700 - 815 °C1290 - 1500 °F
Hot-Working Temperature 825 - 950 °C1520 - 1740 °F
 
Component Elements PropertiesMetricEnglishComments
Copper, Cu 98.7 - 99.19 %98.7 - 99.19 %
Iron, Fe 0.80 - 1.2 %0.80 - 1.2 %
Phosphorus, P 0.010 - 0.040 %0.010 - 0.040 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Copper, UNS C19200, H06 Temper strip
Overview of materials for Copper Alloy
Oxygen-free Copper (OF), UNS C10200, H01 Temper, flat products
Phosphorus deoxidized tellurium bearing Copper, UNS C14500, H02 Temper 6 mm and 13 mm rods
Phosphorus deoxidized tellurium bearing Copper, UNS C14500, OSO15 Temper 13 mm rod

MC19200b6 / 10931

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.