MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Versalis Europrene® SOL T 177 Styrene - Butadiene Block Copolymer
Categories: Polymer; Thermoplastic; Styrene-Butadiene; Styrene/Butadiene/Styrene (SBS)

Material Notes: Europrene® SOL T 177 is a radial block copolymer obtained by anionic polymerization. The polymer is based on styrene and butadiene, where bound styrene is 50% weight. The polymer is extended with paraffinic oil (40 phr). A non-staining antioxidant system is added during the production process.

Key Features: Europrene® SOL T 177 is a block copolymer with radial structure, providing excellent mechanical properties, high strength and elasticity in a wide range of formulated products. The oil addition allows good flow characteristics.

Main Applications: Used as a high strength base in formulated compounds for footwear, the grade is specifically designed for high hardness compounds.

Information provided by Polimeri Europa. Mechanical properties measured on ASTM D 4703 compression molded samples.

Versalis is the Eni subsidiary containing the plastics and rubber businesses.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.940 g/cc0.940 g/ccASTM D792
Melt Flow 15 g/10 min
@Load 5.00 kg,
Temperature 190 °C
15 g/10 min
@Load 11.0 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 8686ASTM D2240
Tensile Strength at Break 15.0 MPa2180 psiASTM D412
Elongation at Break 950 %950 %ASTM D412
300% Modulus 3.00 MPa
@Strain 300 %
435 psi
@Strain 300 %
ASTM D412
Abrasion 170170[mm³]; DIN 53516

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Versalis Europrene® SOL T 172 Styrene - Butadiene Block Copolymer
Versalis Europrene® SOL T 6306 Styrene - Butadiene Block Copolymer
Total Finaprene® 409 Thermoplastic Elastomer
Versalis Europrene® SOL T 161B Styrene - Butadiene Block Copolymer
Versalis Europrene® SOL T 161C Styrene - Butadiene Block Copolymer

PENG207 / 124601

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.