MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Huntsman AVALON® 60 AE-ESD Thermoplastic Polyurethane
Categories: Polymer; Thermoplastic; Polyurethane, TP; Thermoplastic Polyurethane (TPUR), Polyester Grade

Material Notes: AVALON® ESD range are soft TPUs that deliver the improved bonding strength and mechanical properties required to produce high-quality footwear on roundtable machines – specifically safety shoes that must demonstrate anti-static (ESD) properties. The AVALON® ESD products combine softness with flexural strength. The result is shoes and boots that are comfortable yet hard wearing enough to withstand challenging conditions.

Performance Features: AVALON® injection molding products are trusted worldwide to deliver:

  • Outstanding flex performance
  • Excellent slip resistance
  • Perfect surface definition
  • Transparency and translucency
  • Oil resistance
  • Fast cycle times
  • Outstanding abrasion and scratch resistance
  • Perfect color match with masterbatches
  • Rubber-like look and feel
  • Excellent bonding.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.20 g/cc0.0434 lb/in³ISO 2781
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 6060ISO 868
Tensile Strength at Break 16.0 MPa2320 psiISO 37
Elongation at Break 1000 %1000 %ISO 37
100% Modulus 2.40 MPa
@Strain 100 %
348 psi
@Strain 100 %
ISO 37
300% Modulus 3.80 MPa
@Strain 300 %
551 psi
@Strain 300 %
ISO 37
Tear Strength 40.0 kN/m228 pliISO 34B
Abrasion 8080mm3; ISO 4649
 
Electrical PropertiesMetricEnglishComments
Surface Resistance 1.00e+8 ohm1.00e+8 ohm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Huntsman AVALON® 65 AE Thermoplastic Polyurethane
Huntsman AVALON® 60 ABX Thermoplastic Polyurethane
BASF Elastollan® B 60 A WHA TPUR
BASF Elastollan® B 60 A ESD TPUR
Huntsman AVALON® 55 AEX Thermoplastic Polyurethane

PHUQ166 / 159539

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.