MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Lubrizol Stat-Rite® M-809 Static Control Acrylic
Categories: Polymer; Thermoplastic; Acrylic (PMMA); Acrylic, General Purpose, Molded

Material Notes: Stat-Rite® M-809 is a static dissipative Acrylic alloy. Stat-Rite® M-809 utilizes the patented Stat-Rite® inherently dissipative polymer (IDP) alloy system to provide clean, permanent ESD protection. Stat-Rite® IDP alloys provide consistent static dissipation even when extruded, injection molded or thermoformed into components.

Features:

  • Permanent static dissipative performance
  • Humidity insensitive
  • Recyclable and reusable

Applications:

  • Thermoformed packaging
  • PCB trays
  • Electronic component packaging

Properties of all Stat-Rite® polymer products in the molten state are adversely affected by moisture. Although Stat-Rite® compounds are dry when packaged, trace amounts of moisture can be absorbed during storage and handling. For best results, always dry the material three to four hours at 70°C (160°F) in a dehumidifying hopper dryer.

Available in Americas, Europe, Middle East, Africa, India and Asia

Data provided by Lubrizol

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.11 g/cc0.0401 lb/in³ASTM D792
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 26.2 MPa3800 psiASTM D638
Elongation at Break 27 %27 %ASTM D638
Tensile Modulus 1.51 GPa219 ksiASTM D638
Flexural Modulus 1.45 GPa210 ksiASTM D790-92
Izod Impact, Notched 1.39 J/cm2.60 ft-lb/inASTM D256-92
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+10 ohm-cm1.00e+10 ohm-cmASTM D257
Surface Resistance 9.00e+9 ohm9.00e+9 ohm12% RH; ESD S11.11
Surface Resistivity per Square 1.00e+10 ohm1.00e+10 ohm50% RH; ASTM D257
Static Decay 0.030 sec0.030 secFTMS-101C; 12% R.H. (+5000 V to 50 V)
 0.040 sec0.040 secFTMS-101C; 12% R.H. (-5000 V to -50 V)
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 75.0 °C167 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 67.0 °C153 °FASTM D648
 
Descriptive Properties
ColorTransparent

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Lubrizol Stat-Rite® M-690 Static Control PETG Alloy
Lubrizol STAT-RITE® X-5091 Ether-Type Static Dissipative Polymer
Lubrizol Isoplast® 101 Engineering Thermoplastic Polyurethane Resin
RTP Company PermaStat® 301 FR Polycarbonate (PC), ESD Protection - Permanently Anti-static - Glass Fiber - Flame Retardant
Lubrizol Stat-Rite® X-5111 Static Control Polypropylene

PNOVEON20 / 55453

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.