Cotronics Duralco™ 133 500°F (260°C) Aluminum Filled Epoxy
Categories:
Polymer
;
Thermoset
;
Epoxy
Material Notes:
Two component, heat curing, aluminum filled epoxy suitable for high temperature tooling and a readily machinable repair or construction material. Similar to Duralco™ 132, but with a maximum service temperature of 600°F (315°C). Cures with mild heat.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Viscosity
28000
cP
28000
cP
Electrical Properties
Metric
English
Comments
Volume Resistivity
1.00e+6
ohm-cm
1.00e+6
ohm-cm
Thermal Properties
Metric
English
Comments
Thermal Conductivity
5.76
W/m-K
40.0
BTU-in/hr-ft²-°F
Maximum Service Temperature, Air
316
°C
600
°F
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
Cotronics Duralco™ 132 500°F (260°C) Aluminum Filled Epoxy
Cotronics Duralco™ 125 450°F Stress Free, Silver Filled Epoxy, Thermally Conductive
Cotronics Duralco™ 135 500°F (260°C) Aluminum Filled Epoxy
Cotronics Resbond™ 950 High Temperature Ceramic Adhesive, Aluminum Composition
Solvay EF5313 Polysiloxane Polymer
PCOTR0362 / 29059
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.