MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Meldin Supplier

DuPont Mobility and Materials Vespel® ASB-0670 Metal-Back Composite
Categories: Polymer

Material Notes: DuPont™ Vespel® ASB-0670 parts are metal backed to offer enhanced load-carrying capacity, while providing a self-lubricating composite surface. The fabric component of ASB-0670 provides a low coefficient of friction and high strength to achieve superior wear life

Information provided by DuPont. This product line has remained with DuPont after the DuPont-Dow merger.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Coefficient of Friction, Dynamic  0.020
@Pressure 500 MPa
0.020
@Pressure 72500 psi
Rub Velocity: 58 mm/sec
 0.030
@Pressure 500 MPa
0.030
@Pressure 72500 psi
Rub Velocity: 37 mm/sec
 0.030
@Pressure 600 MPa
0.030
@Pressure 87000 psi
Rub Velocity: 60 mm/sec
 0.030
@Pressure 300 MPa
0.030
@Pressure 43500 psi
Rub Velocity: 55 mm/sec
 0.030
@Pressure 200 MPa
0.030
@Pressure 29000 psi
Rub Velocity: 90 mm/sec
 0.040
@Pressure 600 MPa
0.040
@Pressure 87000 psi
Rub Velocity: 12 mm/sec
 0.040
@Pressure 200 MPa
0.040
@Pressure 29000 psi
Rub Velocity: 55 mm/sec
 0.040
@Pressure 300 MPa
0.040
@Pressure 43500 psi
Rub Velocity: 14 mm/sec
 0.040
@Pressure 500 MPa
0.040
@Pressure 72500 psi
Rub Velocity: 20 mm/sec
 0.050
@Pressure 500 MPa
0.050
@Pressure 72500 psi
Rub Velocity: 6 mm/sec
 0.050
@Pressure 200 MPa
0.050
@Pressure 29000 psi
Rub Velocity: 30 mm/sec
 0.060
@Pressure 200 MPa
0.060
@Pressure 29000 psi
Rub Velocity: 3 mm/sec
 0.035
@# of Cycles 0.000
0.035
@# of Cycles 0.000
 0.40
@# of Cycles 13000
0.40
@# of Cycles 13000
Coefficient of Friction, Static  0.0375
@Pressure 450 MPa
0.0375
@Pressure 65300 psi
 0.038
@Pressure 200 MPa
0.038
@Pressure 29000 psi
 
Descriptive Properties
Wear Factor30000 mmDistance rubbed until substrate contact at 400 MPa
 300000 mmDistance rubbed until substrate contact at 200 MPa
 75000 mmDistance rubbed until substrate contact at 300 MPa

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
DuPont Mobility and Materials VESPEL TP-8130 Polyimide
DuPont Mobility and Materials VESPEL TP-8054 Polyimide
TIMCAL TIMREX® T800 Primary Synthetic Graphite
DuPont Mobility and Materials Vespel® SP-1 ISO Polyimide
Chevron Phillips Marlex® 5430 Low Density Polyethylene, Cast Film

PDU2061m / 183714

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.