Description: Vinylbond 96-1050-21 BLACK is a flexible vinyl extrusion compound formulated specifically for the window market industry. This particular compound offers excellent bonding characteristics to ABS and PETG which makes it ideal for coextrusion applications. Information provided by Colorite Polymers. |