MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Ceradyne Thermo-Sil® Castable 220 Fused Silica  (discontinued **)
Categories: Ceramic; Oxide; Silicon Oxide

Material Notes: Fused Silica is an excellent thermal insulator with an extremely low coefficient of thermal expansion. It is excellent for thermal shock applications. The key characteristics of this material are:
  • High Thermal Shock Resistance
  • Radio wave, IR & Microwave Transparent
  • Information provided by Ceradyne Company

    Ceradyne was acquired by 3M in 2012. The product line has been extensively renamed and reconfigured.

    Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
     
    Physical PropertiesMetricEnglishComments
    Bulk Density 2.06 - 2.12 g/cc0.0744 - 0.0766 lb/in³
    Water Absorption 13 - 15 %13 - 15 %ASTM C20
    Porosity 13 - 15 %13 - 15 %ASTM C20
    Crystallinity <= 2.0 %<= 2.0 %
     
    Mechanical PropertiesMetricEnglishComments
    Modulus of Rupture 0.0103 - 0.0124 GPa1.49 - 1.80 ksiASTM C133
    Flexural Strength 10.3 - 12.4 MPa1490 - 1800 psi
    Compressive Strength 48.3 - 51.7 MPa7010 - 7500 psiASTM C133
     
    Thermal PropertiesMetricEnglishComments
    CTE, linear 1.70 µm/m-°C
    @Temperature 20.0 °C
    0.944 µin/in-°F
    @Temperature 68.0 °F
    Thermal Conductivity 0.720 W/m-K5.00 BTU-in/hr-ft²-°F
    Shrinkage 0.0 %
    @Temperature 1100 °C
    0.0 %
    @Temperature 2010 °F
     
    Optical PropertiesMetricEnglishComments
    IR Transmittance 90 %90 %transparent; thickness not quantified
    UV Transmittance 90 %90 %transparent; thickness not quantified

    **
    Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

    Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

    Users viewing this material also viewed the following:
    Ceradyne Thermo-Sil® Castable TG Fused Silica
    Ceradyne Thermo-Sil® Castable 120 Fused Silica
    Ceradyne Thermo-Sil® UHS Fused Silica
    Mateck Fused Silica UV-VIS Grade (SiO2)
    Ceradyne Thermo-Sil® HS Fused Silica

    CCERDN33 / 716

    Aluminum Castings

    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.