MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

USP Class VI adhesives

Multibase C6-560 Dow-Corning Class VI Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes:

Information provided by Multibase

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.10 g/cc0.0397 lb/in³Relative, no post cure; ASTM D792
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 5858no post cure; ASTM D2240
 5858post cured-2 hours at 177°C; ASTM D2240
 5959post cured-4 hours at 177°C; ASTM D2240
 5959post cured- 8 hours at 177°C; ASTM D2240
Tensile Strength, Ultimate 8.55 MPa1240 psipost cured- 8 hours at 177°C; ASTM D412
 8.784 MPa1274 psipost cured- 4 hours at 177°C; ASTM D412
 8.798 MPa1276 psipost cured- 2 hours at 177°C; ASTM D412
 8.83 MPa1280 psino post cure; ASTM D412
Tensile Strength, Yield 3.96 MPa575 psiat 200%, no post cure- press cured for 5 minutes; ASTM D412
 4.21 MPa610 psi200%, post cured- 4 hours at 177°C; ASTM D412
 4.27 MPa619 psiat 200%, post cured- 2 hours at 177°C; ASTM D412
 4.29 MPa622 psi200%, post cured- 8 hours at 177°C; ASTM D412
Elongation at Break 492 %492 %post cured- 8 hours at 177°C; ASTM D412
 503 %503 %post cured- 2 hours at 177°C; ASTM D412
 518 %518 %post cured- 4 hours at 177°C; ASTM D412
 540 %540 %no post cure; ASTM D412
Tear Strength 47.5 kN/m271 pliDie B, post cured- 2 hours at 177°C; ASTM D624
 49.4 kN/m282 pliDie B, post cured- 4 hours at 177°C; ASTM D624
 50.7 kN/m289 pliDie B, post cured- 8 hours at 177°C; ASTM D624
 50.8 kN/m290 pliDie B, no post cure; ASTM D624
Compression Set 33 %33 %no post cure; ASTM D395
 
Thermal PropertiesMetricEnglishComments
Shrinkage 2.7 %2.7 %no post cure
 
Compliance PropertiesMetricEnglishComments
USP Class VI YesYes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Westlake Plastics Radel® R 5500 Polyphenylsulfone For Medical Applications
Blood Plasma
Multibase C6-515 Dow-Corning Class VI Elastomer
Dow Silastic® 1604-T SILICONE RUBBER
Dow Silastic® Q7-4720 BIOMEDICAL GRADE ETR ELASTOMER, KIT

PMULTI180 / 54084

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.