MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Celanese 1000 Nylon 6/6, Dry As Molded  (discontinued **)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Unreinforced, Flame Retardant

Material Notes: General purpose

Information provided by Celanese Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.14 g/cc0.0412 lb/in³ASTM D792
Water Absorption 1.5 %1.5 %ASTM D570
Linear Mold Shrinkage, Flow 0.016 cm/cm0.016 in/in
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 8080ASTM D785
Tensile Strength, Ultimate 83.0 MPa12000 psiASTM D638
Tensile Strength, Yield 83.0 MPa12000 psiASTM D638
Elongation at Break 40 - 80 %40 - 80 %ASTM D638
Flexural Strength 117 MPa17000 psiASTM D790
Flexural Modulus 2.90 GPa421 ksiASTM D790
Shear Strength 66.0 MPa9570 psiASTM D732
Izod Impact, Notched 0.500 J/cm0.937 ft-lb/inASTM D256
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 1.00e+14 ohm-cm1.00e+14 ohm-cmASTM D257
Dielectric Strength 24.0 kV/mm610 kV/inShort Time; ASTM D149
 
Thermal PropertiesMetricEnglishComments
CTE, linear 90.0 µm/m-°C
@Temperature 20.0 °C
50.0 µin/in-°F
@Temperature 68.0 °F
ASTM D696
Melting Point 257 °C495 °FASTM D789
Deflection Temperature at 0.46 MPa (66 psi) 243 °C469 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 88.0 °C190 °FASTM D648
Flammability, UL94 V-2
@Thickness 1.60 mm
V-2
@Thickness 0.0630 in

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Celanese 1000 Nylon 6/6, at 50% RH
Bamberger Polymers Bapolene® 1052 Polyethylene, Injection Grade
Ascend Performance Materials Vydyne® 47H NT Impact Modified Nylon 66
Ascend Performance Materials Vydyne® 47H BK0668 Impact Modified Nylon 66
Overview of materials for Low Density Polyethylene (LDPE), Molded

PHCT39 / 45679

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.