MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Versalis Dutral® PM 06 PLE Ethylene - Propylene Masterbatch
Categories: Other Engineering Material; Additive/Filler for Polymer; Polymer

Material Notes: Dutral® PM 06 PLE is a masterbatch based on Ethylene - Propylene elastomer produced by suspension polymerization using a Ziegler-Natta Catalyst. A non-staining antioxidant is added during the production process.

Key Features: Dutral® elastomers are characterized by excellent resistance to ageing and weathering, good resistance to both high an low temperatures, low permanent set values, good resistance to a large number of chemicals. Dutral® PM 06 PLE is a masterbatch suitable for polyolefin modification, especially low flow PP(MFI (230°C/2.16kg) = 1-10 g/10 mins).

Main Applications: Polymer modification.

Information provided by Polimeri Europa.

Versalis is the Eni subsidiary containing the plastics and rubber businesses.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Volatiles <= 0.20 %<= 0.20 %
Melt Flow 1.8 g/10 min
@Load 5.00 kg,
Temperature 230 °C
1.8 g/10 min
@Load 11.0 lb,
Temperature 446 °F
Ash <= 0.30 %<= 0.30 %
 
Descriptive Properties
Pellets Size0.45 gwt of 30 pellets

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Trelleborg E602 EPDM Rubber
Vicone High Performance Rubber VicoSeal™ 07EK-BK High Performance EPDM Rubber
Trelleborg E450 EPDM Rubber
Trelleborg E350 EPDM Rubber
Rubatex R495 EPDM Rubber Foam Sheet

PENG232 / 124626

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.