MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

TIMCAL TIMREX® KS150-600SP Primary Synthetic Graphite
Categories: Carbon; Graphite; Other Engineering Material; Additive/Filler for Polymer

Material Notes: TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all production and processing stages, strict final inspection, and clearly defined development processes.

TIMREX Primary Synthetic Graphite shows unique properties thanks to the combination of a consistent purity, perfect crystalline structure and well defined texture.

Applications:

  • Copper friction parts copper clutch facings
Information provided by TIMCAL

Key Words: CAS Number 7782-42-5
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.670 g/cc0.0242 lb/in³Scott
 0.770 g/cc0.0278 lb/in³Tap
Particle Size >= 250 µm>= 250 µmd50, 83%, Vibrated sieving
 >= 500 µm>= 500 µmd90, 22%, Vibrated sieving
 550 µm550 µmat a density of 2.16 g/cc
 1000 µm1000 µmat a density of 2.12 g/cc
Deformation 1.4 %1.4 %elastic
 1.4 %1.4 %plastic
 2.8 %2.8 %plastic + elastic
Ash 0.060 %0.060 %Typical
 
Mechanical PropertiesMetricEnglishComments
Coefficient of Friction 0.59
@Temperature 850 °C,
Time 10800 sec
0.59
@Temperature 1560 °F,
Time 3.00 hour
Sintered Cu-C -brake pads with 10% TIMREX® Coke, Sinter density: 55% of the theoret. density
Abrasion 0.25
@Temperature 850 °C,
Time 10800 sec
0.25
@Temperature 1560 °F,
Time 3.00 hour
Friction coefficient and wear of sintered Cu-C -brake pads with 10% T 150-600 Graphite, Sinter density: 55% of theoretical
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 140 W/m-K972 BTU-in/hr-ft²-°F
 
Component Elements PropertiesMetricEnglishComments
H2O, Water 0.040 %0.040 %Typical
 
Descriptive Properties
Crystallite height Lc>100 nm
DBP absorption17 g/100g(Dibutylphthalate)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
TIMCAL TIMREX® KS300-1250 Primary Synthetic Graphite
TIMCAL TIMREX® KS500 Primary Synthetic Graphite
Graphite, Carbon, C
NeoGraf eGRAF® HITHERM™ HT-2505 Graphite with Polymer Additive
NeoGraf eGRAF® HITHERM™ HT-2510 Graphite with Polymer Additive

CTIMCAL18 / 2660

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.